1.
Braz. dent. sci ; 25(1): 1-19, 2022. tab, ilus
Article in English | LILACS, BBO | ID: biblio-1354195

ABSTRACT

Increased patient demands for highly esthetic implant superstructure in the anterior esthetic zone has increased in the last decades. Moreover, the absence of periodontal ligament in implant supported prosthesis causes forces to be transferred without cushioning effect to the alveolar bone, resulting in increased marginal bone loss (MBL) and influence the heath of peri-implant tissue. Evaluate the available evidence on the effect implant superstructure and it consequences on patient satisfaction, MBL, bleeding on probing (BOP) and probing depth (PD). A protocol of electronic and hand research was performed for English based researches comparing implants inserted in the esthetic zone with all ceramic superstructure: "Will the use of different types of all ceramic superstructure show different esthetic patient satisfaction, marginal bone loss, bleeding on probing and probing depth? Thirteen publications from one thousand one hundred and sixteen research studies were included. This systematic review showed that all ceramic implant superstructure was a versatile treatment option with higher esthetic patient satisfaction and better color of peri-implant mucous especially in patients having thin biotype. On the other hand there wasn't significant difference in MBL, PD and BOP compared to other conventional implant superstructure. More randomized controlled clinical trials with bigger samples are needed to confirm our findings. All ceramic implant superstructure is versatile and highly esthetic treatment option for implant placed in the anterior esthetic zone.(AU)


A demanda do paciente por superestruturas de implante altamente estéticas na zona anterior aumentou nas últimas décadas. Além disso, a ausência de ligamento periodontal em próteses implantossuportadas faz com que as forças sejam transferidas para o osso alveolar sem amortecimento, resultando em aumento da perda óssea marginal (MBL) e influenciando na saúde do tecido peri-implantar. Avaliar as evidências disponíveis sobre o efeito da superestrutura do implante e suas consequências na satisfação do paciente, perda óssea marginal, sangramento à sondagem (SS) e profundidade de sondagem (PS). Um protocolo de pesquisa eletrônica e manual foi realizado para a análise de artigos em inglês comparando implantes com toda a superestrutura em cerâmica inseridos na zona estética: "O uso de diferentes tipos de superestrutura em cerâmica mostrará diferentes níveis de satisfação estética do paciente, perda óssea marginal, sangramento em profundidade de sondagem e sondagem?". Foram selecionadas 1116 publicações e apenas treze estudos foram incluídos na análise final. Esta revisão sistemática mostrou que toda superestrutura do implante em cerâmica foi uma opção de tratamento versátil, com maior satisfação estética do paciente e melhor coloração da mucosa peri-implantar, especialmente em pacientes com biótipo fino. Por outro lado, não houve diferença significativa em MBL, PS e SS em comparação com outras superestruturas de implantes convencionais. Porém, mais ensaios clínicos controlados randomizados com amostras maiores são necessários para confirmar nossos achados. Implicações clínicas: Toda superestrutura do implante em cerâmica é uma opção de tratamento versátil e altamente estética para implantes colocados na zona anterior (AU)


Subject(s)
Alveolar Bone Loss , Patient Satisfaction , Esthetics, Dental
2.
Braz. dent. sci ; 24(3): 1-14, 2021. tab, ilus
Article in English | BBO, LILACS | ID: biblio-1282177

ABSTRACT

Objective: To evaluate fracture resistance and survival rate of IPS Empress CAD versus Polished Celtra Duo ceramic laminate veneers. Material and Methods:Thirty-six ceramic laminate veneers were fabricated for maxillary anterior teeth. The patients were divided into two groups according to the material Group 1(control group) fabricated from IPS Empress CAD laminate veneers and group 2 (intervention group) fabricated from Polished Celtra Duo laminate veneers. Standardized the same preparation with butt joint design and chamfer finish line located supra gingival were performed for all the teeth. The fabrication of the veneers was performed using Cad\Cam (Ceramill motion) machine, with software (Exocad). The veneers surfaces were treated and silanated according to the manufacture instruction of each ceramic and enamel surfaces were etched where total etch adhesive protocol was obeyed using BISCO. Follow up sessions were done every two months up to one year for each patient using dental probe and operator vision to evaluate the fracture, survival rate, marginal adaptation, sensitivity and caries. according to USPHS criteria (United States Public Health Service). This was performed by an experienced, blinded investigator. Results: Fracture resistance, marginal adaptation, retention, caries and sensitivity were evaluated according to the criteria of USPHS and we found there is no significant difference as both groups scaled zero score. Conclusion: Both IPS Empress Cad and Polished Celtra Duo laminate veneers revealed successful clinical performance in terms of fracture resistance, marginal adaptation, retention, and sensitivity after one year follow up period (AU)


Objetivo: Avaliar a resistência à fratura e a taxa de sobrevivência de laminados de cerâmica IPS Empress CAD versus Celtra Duo polidos. Material e Métodos: Trinta e seis facetas cerâmicas laminadas foram confeccionadas para dentes anteriores superiores. Os pacientes foram divididos em dois grupos de acordo com o material Grupo 1 (grupo controle) confeccionado com laminados IPS Empress CAD e grupo 2 (grupo intervenção) confeccionado com laminados Celtra Duo polidos. A mesma forma de preparo e acabamento de chanfro localizado supra-gengival padronizados foram realizados para todos os dentes. A confecção das facetas foi realizada em máquina Cad \ Cam (Ceramill motion), com software (Exocad). As superfícies laminadas foram tratadas e silanizadas de acordo com as instruções do fabricante de cada cerâmica e as superfícies de esmalte foram condicionadas seguindo o protocolo adesivo de condicionamento ácido total com BISCO. Sessões de acompanhamento foram realizadas a cada dois meses durante um ano para cada paciente usando sonda exploradora e visão do operador para avaliar a fratura, taxa de sobrevivência, adaptação marginal, sensibilidade e cárie; de acordo com os critérios USPHS (Serviço de Saúde Pública dos Estados Unidos). Isso foi realizado por um investigador experiente e cego. Resultados: a resistência à fratura, adaptação marginal, retenção, cárie e sensibilidade foram avaliadas de acordo com os critérios da USPHS e não encontramos diferença significativa, pois ambos os grupos escalonaram pontuação zero. Conclusão: As facetas laminadas IPS Empress Cad e Celtra Duo polido revelaram desempenho clínico bem-sucedido em termos de resistência à fratura, adaptação marginal, retenção e sensibilidade após um período de acompanhamento de um ano. (AU)


Subject(s)
Humans , Dental Marginal Adaptation , Dental Caries , Dental Veneers , Dentin Sensitivity , Flexural Strength