Chinese Journal of Stomatology ; (12): 296-299, 2016.
Artículo en Chino | WPRIM | ID: wpr-259410

RESUMEN

<p><b>OBJECTIVE</b>To evaluate the adaptation of different lithium disilicate glass-ceramic crown and whether different fabrication processes affect the adaptation of crowns.</p><p><b>METHODS</b>Thirty epoxy dies crowns were divided into 3 groups. They were cemented to domestic lithium disilicate glass-ceramic crowns in Group A, to IPS e.max CAD crowns in Group B and to IPS e.max Press crowns in Group C respectively. All crowns were cut by cutting machine. A confocal laser scanning microscope was used to measure the gap between crown tissue surface and die.</p><p><b>RESULTS</b>There were significant differences in the three groups of measurement points(P<0.05). Within the groups, specimens in group A showed in the lowest marginal fit([46.8±9.1] μm). Those in group B showed the lowest shoulder suitability([59.3±7.9] μm), axial plane([50.5±3.6] μm) and occlusal surface([87.6±11.6 μm]. Those in group C demonstrated the lowest axial plane angle[(84.4±10.1) μm]. In addition to the axial plane angle, the CAD/CAM system exhibited good accuracy of fit.</p><p><b>CONCLUSIONS</b>The three groups of lithium disilicate glass-ceramic crowns appeared to have clinically acceptable fit.</p>


Asunto(s)
Humanos , Cerámica , Diseño Asistido por Computadora , Coronas , Adaptación Marginal Dental , Porcelana Dental , Diseño de Prótesis Dental , Métodos , Microscopía Confocal , Propiedades de Superficie
SELECCIÓN DE REFERENCIAS
DETALLE DE LA BÚSQUEDA