A poly( GMA-EGDMA) coated SPME fiber was prepared using an in-situ polymerization by direct bonding to the surface of a polydopamine-modified stainless steel wire. Then the fiber was modified by sulfuric acid. A novel solid phase microextraction coating coupled to high performance liquid chromatography ( HPLC) method based on the as-prepared fiber was developed for the determination of four pharmaceuticals and personal care products ( PPCPs) in water samples. The influences of extraction parameters, including pH, extraction time, extraction temperature and salt addition were investigated. 3 mL water sample was extracted by the as-prepared fiber for 60 min at 30 ℃, and then desorbed with mobile phase for 30 min, respectively. Desorption solution was analyzed by HPLC-DAD ( diode array detection ) . The results indicated that the extraction yield of the fiber was good for four PPCPs. The linear correlation coefficients were>0. 997 with the linear range of 2-200 μg/L. The limits of detection (S/N=3) were 0. 5-5 μg/L with RSD (n=5) of 4. 1%-11. 9%. The recoveries of four PPCPs at spiked level of 20, 50, 100 μg/L were within the range of 70. 6%-105. 5%. The results showed that this method was easy, green, accurate and precise, and could be used to assay the four PPCPs in real water samples.

SELECCIÓN DE REFERENCIAS
DETALLE DE LA BÚSQUEDA