Determinar la cantidad de degradación de fuerzas en cadenas elastoméricas de dos marcas diferentes. Materiales y métodos. Se elaboraron quince muestras de cada marca comercial de cadenas elastoméricas (American Orthodontics y Denstply GAC) de cuatro eslabones cada una, transparentes y de tipo short. Se confeccionaron bases acrílicas en las cuales se insertaron y fijaron pines metálicos que tuvieron como finalidad mantener las muestras permanentemente traccionadas a una distancia de 15 mm. Se midió la fuerza de tracción inicial utilizando un dinamómetro calibrado. Las muestras fueron sumergidas en saliva artificial. Un solo investigador realizó el mismo procedimiento en intervalos de 1 día, 7 días, 14 días y 21 días. Resultados. Para comparar la degradación de fuerzas de ambos grupos se emplearon las pruebas U de Mann-Whitney y t de Student a un nivel de significancia de 5%. Al inicio del estudio hubo una diferencia muy significativa (p<0,001). A las 24 h se mantuvo la diferencia significativa (p<0,024). A los 7 días no hubo diferencia significativa (p<0,299). Pero, a los 14 días hubo una diferencia muy significativa (p<0,001) y a los 21 días hubo diferencia altamente significativa (p<0,001). Conclusiones. Se encontró que ambas marcas comerciales mostraron una alta degradación de fuerzas al primer día. Posteriormente, la degradación de fuerzas de cada muestra disminuyó en intensidady fue más estable. La marca Denstply GAC frente a la marca American Orthodontics, mostró mayor cantidad de fuerza remanente al final del estudio...


To determine the amount of degradation force in elastomeric chains of two different brands. Materials and methods. Fifteen samples of each brand of elastomeric chains (American Orthodontics y Denstply GAC) of four brands each, transparent and short type were manufactured. Acrylic bases in which metal pins were inserted and fixed that had the objective to keep the samples permanently drivable at a distance of 15 mm were prepared. Initial tensile strength was measured using a calibrated dynamometer. Samples were immersed in artificial saliva. A single investigator performed the same procedure in 1 day, 7 days, 14 days and 21 days. Results. To compare the degradation of forces of both groups U Mann-Whitney test and Student t test at a significance level of 5% were used. At baseline there was a significant difference (p <0,001). At 24 h the significant difference (p <0,024) remained. At 7 days, there was no significant difference (p <0,299). But, at 14 days there was a highly significant difference (p <0,001) and 21 days there were highly significant (p <0,001). Conclusions. It was found that both brands showed high force degradation the first day. Subsequently, force degradation of each sample was decreased in intensity and was more stable. The brand Denstply GAC in comparison to the mark American Orthodontics showed greater amount of force remaining at the end of the study...


Assuntos
Aparelhos Ativadores , Elastômeros , Procedimentos de Ancoragem Ortodôntica , Ortodontia Corretiva , Estudos Longitudinais , Estudos Prospectivos
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA