The Journal of Korean Academy of Prosthodontics ; : 386-395, 2002.
Artigo em Coreano | WPRIM | ID: wpr-49098

RESUMO

This study would like to measure and compare water sorption and solubility of acrylic resins, with 3 different polymerizing methods, and tensile strength between denture base resin and relining resins. For this experiment, 3 different acrylic resins were used; heat polymerizing resin: Vertex (Dentmex, Zeist,Holland), autopolymerizing resin: Tokuso Rebase (Tokuyama Corp, Tokyo, Japan), and light curing resin: Mild Rebaron LC (GC Corp, Tokyo, Japan) The results were as follows; 1. Tokuso Rebase showed the lowest water sorption, followed by Mild Rebaron LC and Vertex. Among resins, there were some signigicant differences (P0.05). About 50% of Rebaron LC showed cohesive fracture. 4. Tensile strength has more decreased after thermocycling than before, but there was no statistical difference (P>0.05).


Assuntos
Resinas Acrílicas , Bases de Dentadura , Dentaduras , Temperatura Alta , Polímeros , Solubilidade , Resistência à Tração , Água
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA