The Journal of Advanced Prosthodontics ; : 43-52, 2016.
Artigo em Inglês | WPRIM | ID: wpr-211467

RESUMO

PURPOSE: This study was conducted to evaluate the effects of full-coverage all-ceramic zirconia, lithium disilicate glass-ceramic, leucite glass-ceramic, or stainless steel crowns on antagonistic primary tooth wear. MATERIALS AND METHODS: There were four study groups: the stainless steel (Steel) group, the leucite glass-ceramic (Leucite) group, the lithium disilicate glass-ceramic (Lithium) group, and the monolithic zirconia (Zirconia) group. Ten flat crown specimens were prepared per group; opposing teeth were prepared using primary canines. A wear test was conducted over 100,000 chewing cycles using a dual-axis chewing simulator and a 50 N masticating force, and wear losses of antagonistic teeth and restorative materials were calculated using a three-dimensional profiling system and an electronic scale, respectively. Statistical significance was determined using One-way ANOVA and Tukey's test (P.05). CONCLUSION: Leucite glass-ceramic and lithium disilicate glass-ceramic cause more primary tooth wear than stainless steel or zirconia.


Assuntos
Coroas , Lítio , Mastigação , Aço Inoxidável , Aço , Dente , Desgaste dos Dentes , Dente Decíduo
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA