Acta odontol. latinoam ; Acta odontol. latinoam;23(1): 3-7, Apr. 2010. tab
Artigo em Inglês | LILACS | ID: biblio-949628

RESUMO

The aim of this study was to evaluate the clinical behavior of two conventional glass ionomers used for pit and fissure sealing in terms of retention, marginal adaptation, caries recurrence and cracking. Eighty-three fully erupted first permanent molars were sealed, in a group of children aged 5 to 8 years. A doubleblind, single operator, paired design was used. Materials applied were Fuji IX and VII. Retention (R), presence of caries (PC), marginal discoloration (MD), marginal adaptation (MA) and cracking (C) were evaluated at 6 and 12 months using Ryge's criteria. Data registered 6 months after treatment were: Fuji IX: R: Alpha 37, Bravo 2, Charlie: 4; PC: Alpha 43, Bravo: 0; MA: Alpha 38, Bravo: 1; MD: Alpha 39, Bravo: 0, Charlie: 0; C: Alpha 39, Bravo: 0. Fuji VII: R: Alpha 29, Bravo 4, Charlie: 7; PC: Alpha 40, Bravo: 0; MA: Alpha: 34, Bravo: 0; MD: Alpha: 34, Bravo: 0; Charlie: 0; C: Alpha 33, Bravo: 0. Results after one year were: Fuji IX: R: Alpha 33, Bravo: 3, Charlie: 9; PC: Alpha 44, Bravo: 1; MA: Alpha 33, Bravo: 1; MD: Alpha: 34, Bravo: 0, Charlie: 0; C: Alpha: 34, Bravo: 0. Fuji VII: R: Alpha 22, Bravo 4, Charlie: 13, PC: Alpha 40, Bravo: 0; MA: Alpha 23, Bravo: 1; MD: Alpha 23, Bravo: 1, Charlie: 0; C: Alpha 23, Bravo: 1. Statistical analysis using Fisher test showed no significant difference (p>0.05) for R, and MA. For PC, MD and C, values are not reported because both materials showed the same results. The second control showed no significant difference (p>0.05) for R, MA, PC, MD and C. Results suggest no difference between Fuji IX and Fuji VII as sealants in fully erupted permanent molars.


El objetivo de este trabajo fue evaluar el comportamiento clinico de dos ionomeros vitreos convencionales aplicados como selladores de fosas y fisuras. Se evaluo la retencion, decoloracion y adaptacion marginal, incidencia de caries y agrietamiento. Se sellaron ochenta y tres primeros molares totalmente erupcionados en un grupo de ninos de 5 a 8 anos. Se llevo a cabo un diseno de doble ciego, unico operador y apareado. Los materiales aplicados fueron Fuji IX y VII. Luego de 6 y 12 meses se recitaron los ninos y se evaluo: Retencion (R), presencia de caries (PC), decoloracion marginal (MD) y agrietamiento (C). La evaluacion se realizo utilizando los criterios de Ryge. Los datos registrados al cabo de 6 meses fueron: Fuji IX: R: Alpha 37, Bravo 2, Charlie: 4; PC: Alpha 43, Bravo: 0; MA: Alpha 38, Bravo: 1; MD: Alpha 39, Bravo: 0, Charlie: 0; C: Alpha 39, Bravo: 0. Fuji VII: R: Alpha 29, Bravo 4, Charlie: 7; PC: Alpha 40, Bravo: 0; MA: Alpha: 34, Bravo: 0; MD: Alpha: 34, Bravo: 0; Charlie: 0; C: Alpha 33, Bravo: 0. A los 12 meses: Fuji IX: R: Alpha 33, Bravo: 3, Charlie: 9; PC: Alpha 44, Bravo: 1; MA: Alpha 33, Bravo: 1; MD: Alpha: 34, Bravo: 0, Charlie: 0; C: Alpha: 34, Bravo: 0. Fuji VII: R: Alpha 22, Bravo 4, Charlie: 13, PC: Alpha 40, Bravo: 0; MA: Alpha 23, Bravo: 1; MD: Alpha 23, Bravo: 1, Charlie: 0; C: Alpha 23, Bravo: 1. La evaluacion estadistica por medio de la prueba de Fisher no mostro diferencias significativas entre los materiales (p>0.05) para R y MA. En PC, MD y C, el valor de p no se indica ya que los resultados fueron identicos. El segundo control no mostro diferencias significativas (p>0.05) para R, MA, PC, MD y C. Los resultados sugieren que no existiria diferencia en la aplicacion de Fuji IX y Fuji VII como selladores de fosas y fisuras en molares totalmente erupcionados.


Assuntos
Criança , Pré-Escolar , Humanos , Selantes de Fossas e Fissuras , Fissuras Dentárias/terapia , Cimentos de Ionômeros de Vidro , Dente Molar , Método Duplo-Cego