Your browser doesn't support javascript.
loading
Fit of metal-ceramic crowns: effect of coping fabrication method and veneering ceramic application
Kunz, Patrícia Valéria Manozzo; Serpa, Gabriela Andrade; Cunha, Leonardo Fernandes da; Correr, Gisele Maria; Gonzaga, Carla Castiglia.
  • Kunz, Patrícia Valéria Manozzo; Positivo University. School of Health Sciences. Curitiba. BR
  • Serpa, Gabriela Andrade; Positivo University. School of Health Sciences. Curitiba. BR
  • Cunha, Leonardo Fernandes da; University of Brasilia. Department of Dentistry. School of Health Sciences. Brasilia. BR
  • Correr, Gisele Maria; Positivo University. School of Health Sciences. Curitiba. BR
  • Gonzaga, Carla Castiglia; Positivo University. School of Health Sciences. Curitiba. BR
Braz. j. oral sci ; 21: e225136, jan.-dez. 2022. ilus
Article in English | LILACS, BBO | ID: biblio-1354771
ABSTRACT

Aim:

To evaluate the influence of cobalt-chromium (Co-Cr) coping fabrication methods and ceramic application on the marginal and internal fit of metal-ceramic crowns.

Methods:

Co-Cr copings for metal-ceramic crowns were prepared by lost wax casting or CAD-CAM machining of sintered blocks. The fit was analyzed using the silicone replica technique at four assessment points marginal gap (MG), axial wall (AW), axio-occlusal (AO) angle, and central occlusal (CO) wall. After the initial analysis, the copings were ceramic-veneered with the layering technique, and the fit was again determined. Data were statistically analyzed by paired and unpaired Student's-t test (α=0.05).

Results:

Marginal and internal fit before ceramic application according to the coping manufacturing method showed significant differences only at CO (p < 0.001), with milled copings (137.98±16.71 µm) showing higher gap values than cast copings (112.86±8.57 µm). For cast copings, there were significant differences at MG (before 109.13±8.79 µm; after 102.78±7.18 µm) and CO (before 112.86±8.57 µm; after 104.07±10.63 µm) when comparing the fit before and after ceramic firing. For milled copings, there was significant difference only at AO (before 116.39±9.64 µm; after 108.54±9.26 µm).

Conclusion:

This study demonstrated that the coping fabrication method influenced the internal fit. Ceramic firing maintained or improved the fit of the metal-ceramic crowns. The marginal discrepancy of all restorations, before and after ceramic firing, can be considered clinically acceptable
Subject(s)


Full text: Available Index: LILACS (Americas) Main subject: Ceramics / Metal Ceramic Alloys / Dental Marginal Adaptation / Crowns Language: English Journal: Braz. j. oral sci Journal subject: Dentistry Year: 2022 Type: Article Affiliation country: Brazil Institution/Affiliation country: Positivo University/BR / University of Brasilia/BR

Similar

MEDLINE

...
LILACS

LIS


Full text: Available Index: LILACS (Americas) Main subject: Ceramics / Metal Ceramic Alloys / Dental Marginal Adaptation / Crowns Language: English Journal: Braz. j. oral sci Journal subject: Dentistry Year: 2022 Type: Article Affiliation country: Brazil Institution/Affiliation country: Positivo University/BR / University of Brasilia/BR