Your browser doesn't support javascript.
loading
Immediate and delayed solubility of mineral trioxide aggregate and Portland cement
Bodanezi, Augusto; Carvalho, Nara; Silva, Daniela; Bernardineli, Norberti; Bramante, Clovis Monteiro; Garcia, Roberto Brandão; Moraes, Ivaldo Gomes de.
  • Bodanezi, Augusto; University of São Paulo. Bauru School of Dentistry. Department of Operative Dentistry, Endodontics and Dental Materials. Bauru. BR
  • Carvalho, Nara; University of Uberlândia. Uberlândia. BR
  • Silva, Daniela; University of São Paulo. Hospital for Rehabilitation of Craniofacial Anomalies. Bauru. BR
  • Bernardineli, Norberti; University of São Paulo. Bauru School of Dentistry. Endodontics and Dental Materials. Department of Operative Dentistry. Bauru. BR
  • Bramante, Clovis Monteiro; University of São Paulo. Bauru School of Dentistry. Endodontics and Dental Materials. Department of Operative Dentistry. Bauru. BR
  • Garcia, Roberto Brandão; University of São Paulo. Bauru School of Dentistry. Endodontics and Dental Materials. Department of Operative Dentistry. Bauru. BR
  • Moraes, Ivaldo Gomes de; University of São Paulo. Bauru School of Dentistry. Endodontics and Dental Materials. Department of Operative Dentistry. Bauru. BR
J. appl. oral sci ; 16(2): 127-131, Mar.-Apr. 2008. graf, tab
Article in English | LILACS | ID: lil-479758
ABSTRACT
This study investigated the solubility of mineral trioxide aggregate (MTA) and Portland cement since its mixture until 672 hours, by means of two complimentary methods. Metal ring molds filled with the cements were covered with distilled water and, at each experimental time (3, 24, 72, 168, 336 and 672 hours), were weighed as soon as the plates in which the samples have been placed. Empty rings served as the control group (n=8). Mean weight gain and loss was determined and analyzed statistically by two-way ANOVA and Tukey's test for all pairwise comparisons. Only Portland cement showed less than 3 percent weight loss through 24 hours. Detached MTA residues were heavier than those of Portland cement over the 3 to 168 hours. The weight of MTA rings increased more than that of Portland rings within 672 hours (p=0.05). The findings of the present study indicate that, in an aqueous environment MTA is more soluble than Portland cement and exceeds the maximum weight loss considered acceptable by ISO 6876 standard (2001).
Subject(s)

Full text: Available Index: LILACS (Americas) Main subject: Oxides / Root Canal Filling Materials / Silicates / Calcium Compounds / Aluminum Compounds / Dental Cements Limits: Humans Language: English Journal: J. appl. oral sci Journal subject: Dentistry Year: 2008 Type: Article Affiliation country: Brazil Institution/Affiliation country: University of São Paulo/BR / University of Uberlândia/BR

Similar

MEDLINE

...
LILACS

LIS

Full text: Available Index: LILACS (Americas) Main subject: Oxides / Root Canal Filling Materials / Silicates / Calcium Compounds / Aluminum Compounds / Dental Cements Limits: Humans Language: English Journal: J. appl. oral sci Journal subject: Dentistry Year: 2008 Type: Article Affiliation country: Brazil Institution/Affiliation country: University of São Paulo/BR / University of Uberlândia/BR