Resistência à flexão em porcelana feldspática: efeito da ciclagem mecânica e limite de fadiga pelo método escada / Flexural strength of feldspathic porcelain: effect of mechanical cycling and fatigue limit by the staircase method
Schalch, Max Von; Chaves, Carolina de Andrade Lima; Medeiros, Flávia Regina Machado de; Almeida-Júnior, Antonio Alves de; Abi-Rached, Filipe de Oliveira; Cruz, Carlos Alberto dos Santos.
  • Schalch, Max Von; Unesp. FO de Araraquara. Departamento de Materiais Odontológicos. BR
  • Chaves, Carolina de Andrade Lima; Unesp. FO de Araraquara. Departamento de Materiais Odontológicos. BR
  • Medeiros, Flávia Regina Machado de; Unesp. FO de Araraquara. Departamento de Materiais Odontológicos. BR
  • Almeida-Júnior, Antonio Alves de; Unesp. FO de Araraquara. Departamento de Materiais Odontológicos. BR
  • Abi-Rached, Filipe de Oliveira; Unesp. FO de Araraquara. Departamento de Materiais Odontológicos. BR
  • Cruz, Carlos Alberto dos Santos; Unesp. FO de Araraquara. Departamento de Materiais Odontológicos. BR
Rev. bras. odontol ; 70(1): 12-16, Jan.-Jun. 2013. ilus, tab
Article in Portuguese | LILACS | ID: lil-720360
RESUMO
Este estudo avaliou o limite de fadiga (LF), determinado pelo método escada, e o efeito da ciclagem mecânica sobre a resistência à flexão (RF) da porcelana feldspática Duceragold. Corpos de prova (25 x 5 x 2 mm) foram confeccionados de acordo com as instruções do fabricante e submetidos ao ensaio de RF (n = 10), em três pontos. Para determinação do LF (n = 30), foram utilizados carregamento inicial de 60% da RF, tensão incremental de 3% da RF, 10.000 ciclos e 2 Hz. Os dados foram submetidos à Anova e teste de Tukey (p < 0,05). Embora os ciclos propostos não tenham reduzido estatisticamente a RF, análises fractográficas evidenciaram estrias, sinais característicos de fadiga mecânica.
ABSTRACT
This study evaluated the fatigue limit (FL) by the staircase method and the effect of mechanical cycling on the flexural strength (FS) of Duceragold feldspathic porcelain. Specimens (25 x 5 x 2 mm) were made according to manufacturer’s directions and submitted to t hree-point fl exural s trength t est (n = 10). To d etermine FL (n = 30; 10,000 cycles; 2 Hz), an initial loading of 60% of the FS and an incremental loading (step) of 3% of the FS were used. Data were analyzed by Anova and Tukey´s test (p < 0.05). Although the proposed cycles have not reduced FS significantly, fractography analysis showed striation, characteristic signs of mechanical fatigue.
Subject(s)

Full text: Available Index: LILACS (Americas) Main subject: Dental Materials / Dental Porcelain / Materials Science / Flexural Strength Language: Portuguese Journal: Rev. bras. odontol Journal subject: Dentistry Year: 2013 Type: Article Affiliation country: Brazil Institution/Affiliation country: Unesp/BR

Similar

MEDLINE

...
LILACS

LIS

Full text: Available Index: LILACS (Americas) Main subject: Dental Materials / Dental Porcelain / Materials Science / Flexural Strength Language: Portuguese Journal: Rev. bras. odontol Journal subject: Dentistry Year: 2013 Type: Article Affiliation country: Brazil Institution/Affiliation country: Unesp/BR