Your browser doesn't support javascript.
loading
Effects of the combination of Er: YAG laser and sandblasting on the shear bond strength between zirconia and resin cement
Vasconcelos, Urias Silva; Silva, Thalisson Saymo de Oliveira; Silva, Daylana Pacheco da; Silva, Graciela Maria Oliveira; Valente, Valdimar da Silva; Zanetti, Raquel Virginia; Moura, Carmem Dolores Vilarinho Soares de.
Afiliación
  • Vasconcelos, Urias Silva; Federal University of Piauí. School of Dentistry. Teresina. BR
  • Silva, Thalisson Saymo de Oliveira; Federal University of Piauí. School of Dentistry. Teresina. BR
  • Silva, Daylana Pacheco da; Federal University of Piauí. School of Dentistry. Teresina. BR
  • Silva, Graciela Maria Oliveira; Federal University of Piauí. School of Dentistry. Teresina. BR
  • Valente, Valdimar da Silva; University of Federal of Piauí. School of Dentistry. Department of Restorative Dentistry. Teresina. BR
  • Zanetti, Raquel Virginia; University of São Paulo. School of Dentistry. São Paulo. BR
  • Moura, Carmem Dolores Vilarinho Soares de; University of Federal of Piauí. School of Dentistry. Department of Restorative Dentistry. Teresina. BR
Braz. j. oral sci ; 18: e191449, jan.-dez. 2019. ilus
Article en En | LILACS, BBO | ID: biblio-1088047
Biblioteca responsable: BR218.1
ABSTRACT

Aim:

This study was conducted to determine the bond strength between zirconia ceramic and resin luting cement according to the type of surface treatment applied.

Methods:

Sixty zirconia cylinders measuring 4 x 4 mm were manufactured and distributed into five experimental groups and a control group (n = 10) G1 - sandblasting with 110 µm aluminum oxide; G2 - sandblasting with 30 µm Rocatec Soft®; G3 - ErYAG laser irradiation at 400 mJ; G4 - ErYAG laser combined with sandblasting with aluminum oxide; G5 - ErYAG laser combined with sandblasting with Rocatec Soft®; G6 - no treatment (Control). The zirconia cylinders were bonded in the center of composite resin cylinders (6 mm diameter) using RelyX Ultimate® cement. Shear strength was measured after thermocycling (6000 cycles and 5-55° C). Data were analyzed using one-way ANOVA and Tukey's post-hoc with a 5% significance level.

Results:

Group 4 had a significantly higher shear strength than all the other groups, except Group 1. Group 3 had a significantly lower shear strength compared with Groups 1 and 4.

Conclusion:

Sandblasting with 110µm aluminum oxide particles after laser irradiation may be an effective zirconia surface treatment. The use of Er YAG laser alone is not effective at increasing the bond between resin cement and zirconia
Asunto(s)
Palabras clave

Texto completo: 1 Índice: LILACS Asunto principal: Circonio / Resistencia al Corte / Terapia por Láser Idioma: En Revista: Braz. j. oral sci Asunto de la revista: ODONTOLOGIA Año: 2019 Tipo del documento: Article

Texto completo: 1 Índice: LILACS Asunto principal: Circonio / Resistencia al Corte / Terapia por Láser Idioma: En Revista: Braz. j. oral sci Asunto de la revista: ODONTOLOGIA Año: 2019 Tipo del documento: Article