Your browser doesn't support javascript.
loading
Evaluation of phenyl-propanedione on yellowing and chemical-mechanical properties of experimental dental resin-based materials
OLIVEIRA, Dayane Carvalho Ramos Salles de; SOUZA-JUNIOR, Eduardo José; DOBSON, Adam; CORRER, Ana Rosa Costa; BRANDT, William Cunha; SINHORETI, Mário Alexandre Coelho.
  • OLIVEIRA, Dayane Carvalho Ramos Salles de; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Odontologia Restauradora. Piracicaba. BR
  • SOUZA-JUNIOR, Eduardo José; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Odontologia Restauradora. Piracicaba. BR
  • DOBSON, Adam; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Odontologia Restauradora. Piracicaba. BR
  • CORRER, Ana Rosa Costa; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Odontologia Restauradora. Piracicaba. BR
  • BRANDT, William Cunha; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Odontologia Restauradora. Piracicaba. BR
  • SINHORETI, Mário Alexandre Coelho; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Odontologia Restauradora. Piracicaba. BR
J. appl. oral sci ; 24(6): 555-560, Nov.-Dec. 2016. tab, graf
Artículo en Inglés | LILACS, BBO | ID: biblio-841154
ABSTRACT
ABSTRACT Objective To evaluate the influence of phenyl-propanedione on yellowing and chemical-mechanical properties of experimental resin-based materials photoactivated using different light curing units (LCUs). Material and Methods Experimental resin-based materials with the same organic matrix (60:40 wt% BisGMA:TEGDMA) were mechanically blended using a centrifugal mixing device. To this blend, different photoinitiator systems were added in equimolar concentrations with aliphatic amine doubled by wt%: 0.4 wt% CQ; 0.38 wt% PPD; or 0.2 wt% CQ and 0.19 wt% PPD. The degree of conversion (DC), flexural strength (FS), Young’s modulus (YM), Knoop hardness (KNH), crosslinking density (CLD), and yellowing (Y) were evaluated (n=10). All samples were light cured with the following LCUs: a halogen lamp (XL 2500), a monowave LED (Radii), or a polywave LED (Valo) with 16 J/cm2. The results were analysed by two-way ANOVA and Tukey’s test (α=0.05). Results No statistical differences were found between the different photoinitiator systems to KNH, CLS, FS, and YM properties (p≥0.05). PPD/CQ association showed the higher DC values compared with CQ and PPD isolated systems when photoactivated by a polywave LED (p≤0.05). Y values were highest for the CQ compared with the PPD systems (p≤0.05). Conclusion PPD isolated system promoted similar chemical and mechanical properties and less yellowing compared with the CQ isolated system, regardless of the LCU used.
Asunto(s)


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Polietilenglicoles / Ácidos Polimetacrílicos / Bisfenol A Glicidil Metacrilato / Chalconas / Curación por Luz de Adhesivos Dentales / Fotoiniciadores Dentales Tipo de estudio: Estudios de evaluación Idioma: Inglés Revista: J. appl. oral sci Asunto de la revista: Odontología Año: 2016 Tipo del documento: Artículo País de afiliación: Brasil Institución/País de afiliación: Universidade Estadual de Campinas/BR

Similares

MEDLINE

...
LILACS

LIS


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Polietilenglicoles / Ácidos Polimetacrílicos / Bisfenol A Glicidil Metacrilato / Chalconas / Curación por Luz de Adhesivos Dentales / Fotoiniciadores Dentales Tipo de estudio: Estudios de evaluación Idioma: Inglés Revista: J. appl. oral sci Asunto de la revista: Odontología Año: 2016 Tipo del documento: Artículo País de afiliación: Brasil Institución/País de afiliación: Universidade Estadual de Campinas/BR