Does laser diode irradiation improve the degree of conversion of simplified dentin bonding systems?
BRIANEZZI, Leticia Ferreira de Freitas; MAENOSONO, Rafael Massunari; BIM JÚNIOR, Odair; ZABEU, Giovanna Speranza; PALMA-DIBB, Regina Guenka; ISHIKIRIAMA, Sérgio Kiyoshi.
  • BRIANEZZI, Leticia Ferreira de Freitas; Universidade de São Paulo. Faculdade de Odontologia de Bauru. Departamento de Dentística, Endodontia e Materiais Odontológicos. Bauru. BR
  • MAENOSONO, Rafael Massunari; Universidade de São Paulo. Faculdade de Odontologia de Bauru. Departamento de Dentística, Endodontia e Materiais Odontológicos. Bauru. BR
  • BIM JÚNIOR, Odair; Universidade de São Paulo. Faculdade de Odontologia de Bauru. Departamento de Dentística, Endodontia e Materiais Odontológicos. Bauru. BR
  • ZABEU, Giovanna Speranza; Universidade de São Paulo. Faculdade de Odontologia de Bauru. Departamento de Dentística, Endodontia e Materiais Odontológicos. Bauru. BR
  • PALMA-DIBB, Regina Guenka; Universidade de São Paulo. Faculdade de Odontologia de Bauru. Departamento de Dentística, Endodontia e Materiais Odontológicos. Bauru. BR
  • ISHIKIRIAMA, Sérgio Kiyoshi; Universidade de São Paulo. Faculdade de Odontologia de Bauru. Departamento de Dentística, Endodontia e Materiais Odontológicos. Bauru. BR
J. appl. oral sci ; 25(4): 381-386, July-Aug. 2017. tab, graf
Artículo en Inglés | LILACS, BBO | ID: biblio-893641
ABSTRACT
Abstract Simplified dentin-bonding systems are clinically employed for most adhesive procedures, and they are prone to hydrolytic degradation. Objective This study aimed to investigate the effect of laser diode irradiation on the degree of conversion (DC), water sorption (WS), and water solubility (WSB) of these bonding systems in an attempt to improve their physico-mechanical resistance. Material and Methods Two bonding agents were tested: a two-step total-etch system [Adper™ Single Bond 2, 3M ESPE (SB)] and a universal system [Adper™ Single Bond Universal, 3M ESPE (SU)]. Square-shaped specimens were prepared and assigned into 4 groups (n=5): SB and SU (control groups - no laser irradiation) and SB-L and SU-L [SB and SU laser (L) - irradiated groups]. DC was assessed using Fourier transform infrared spectroscopy with attenuated total reflectance. Additional uncured resin samples (≈3.0 µL, n=5) of each adhesive were also scanned for final DC calculation. For WS/WSB tests, similar specimens (n=10) were prepared and measured by monitoring the mass changes after dehydration/water storage cycles. For both tests, adhesive fluids were dropped into standardized Teflon molds (6.0×6.0×1.0 mm), irradiated with a 970-nm laser diode, and then polymerized with an LED-curing unit (1 W/cm2). Results Laser irradiation immediately before photopolymerization increased the DC (%) of the tested adhesives: SB-L>SB>SU-L>SU. For WS/WSB (μg/mm3), only the dentin bonding system (DBS) was a significant factor (p<0.05): SB>SU. Conclusion Irradiation with a laser diode improved the degree of conversion of all tested simplified dentin bonding systems, with no impact on water sorption and solubility.
Asunto(s)


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Recubrimientos Dentinarios / Láseres de Semiconductores / Polimerizacion Tipo de estudio: Estudios de evaluación Idioma: Inglés Revista: J. appl. oral sci Asunto de la revista: Odontología Año: 2017 Tipo del documento: Artículo País de afiliación: Brasil Institución/País de afiliación: Universidade de São Paulo/BR

Similares

MEDLINE

...
LILACS

LIS


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Recubrimientos Dentinarios / Láseres de Semiconductores / Polimerizacion Tipo de estudio: Estudios de evaluación Idioma: Inglés Revista: J. appl. oral sci Asunto de la revista: Odontología Año: 2017 Tipo del documento: Artículo País de afiliación: Brasil Institución/País de afiliación: Universidade de São Paulo/BR