Avaliação do atrito em braquetes autoligáveis submetidos à mecânica de deslizamento: um estudo in vitro / Evaluation of friction in self-ligating brackets subjected to sliding mechanics: an in vitro study
Dental press j. orthod. (Impr.)
;
16(1): 107-115, jan.-fev. 2011. ilus, graf, tab
Artículo
en Portugués
| LILACS
| ID: lil-580321
RESUMO
INTRODUÇÃO:
o atrito gerado na interface braquete/fio durante a mecânica de deslizamento pode reduzir a eficiência da movimentação ortodôntica. O método de ligação do fio ao braquete exerce importante papel na determinação desse atrito.MÉTODOS:
o presente estudo comparou a força de atrito gerada por quatro tipos de braquetes autoligáveis (Time®; Damon 2®; In-Ovation R® e Smart Clip®) com um grupo de braquetes ortodônticos convencionais (Dynalock®) associados a ligaduras elásticas tradicionais (Dispens-A-Stix®), que serviu como grupo controle. A força de atrito estático foi mensurada através da máquina universal de ensaios EMIC® DL 500 com dois fios de aço inoxidável com secção transversal 0,018" e 0,017" x 0,025".RESULTADOS:
a análise de variância ANOVA e o teste de Tukey mostraram baixos níveis de atrito nos quatro braquetes autoligáveis associados ao fio 0,018" (P<0,05). Entretanto, os resultados observados quando os braquetes autoligáveis foram testados com fios 0,017" x 0,025" mostraram alta resistência ao deslizamento nos grupos de braquetes autoligáveis ativos.ABSTRACT
INTRODUCTION:
Friction generated at the bracket/archwire interface during sliding mechanics can reduce the efficiency of orthodontic movement. The ligation method employed to tie the archwire to the bracket plays an important role in determining this friction.METHODS:
This study compared the frictional force generated by four different types of self-ligating brackets (Time, Damon 2, In-Ovation R and Smart Clip) with a group of conventional orthodontic brackets (Dynalock) that require the use of traditional elastomeric ligatures (ExDispens-A-Stix), which served as the control group. Static friction force was measured using an EMIC DL 500 universal testing machine using stainless steel round 0.018-in and rectangular 0.017x0.025-in archwires.RESULTS:
ANOVA and Tukey's test showed low levels of friction in the four self-ligating brackets in tests with the 0.018-in wire (P <0.05). However, the results noted when the self-ligating brackets were tested using 0.017x 0.025-in archwires showed high resistance to sliding in the self-ligating groups.
Texto completo:
Disponible
Índice:
LILACS (Américas)
Asunto principal:
Aparatos Ortodóncicos
/
Soportes Ortodóncicos
/
Fricción
/
Métodos de Anclaje en Ortodoncia
Idioma:
Portugués
Revista:
Dental press j. orthod. (Impr.)
Asunto de la revista:
Ortodoncia
Año:
2011
Tipo del documento:
Artículo
País de afiliación:
Brasil
Institución/País de afiliación:
PUC Minas/BR
Similares
MEDLINE
...
LILACS
LIS