Your browser doesn't support javascript.
loading
Effect of laser welding on the titanium ceramic tensile bond strength
Galo, Rodrigo; Ribeiro, Ricardo Faria; Rodrigues, Renata Cristina Silveira; Pagnano, Valéria de Oliveira; Mattos, Maria da Glória Chiarello de.
  • Galo, Rodrigo; s.af
  • Ribeiro, Ricardo Faria; s.af
  • Rodrigues, Renata Cristina Silveira; s.af
  • Pagnano, Valéria de Oliveira; s.af
  • Mattos, Maria da Glória Chiarello de; s.af
J. appl. oral sci ; 19(4): 301-305, July-Aug. 2011. ilus
Artículo en Inglés | LILACS | ID: lil-599753
ABSTRACT
Titanium reacts strongly with elements, mainly oxygen at high temperature. The high temperature of titanium laser welding modifies the surface, and may interfere on the metal-ceramic tensile bond strength.

OBJECTIVE:

The influence of laser welding on the titanium-ceramic bonding has not yet been established. The purpose of this in vitro study was to analyze the influence of laser welding applied to commercially pure titanium (CpTi) substructure on the bond strength of commercial ceramic. The influence of airborne particle abrasion (Al2O3) conditions was also studied. MATERIAL AND

METHODS:

Forty CpTi cylindrical rods (3 mm x 60 mm) were cast and divided into 2 groups with laser welding (L) and without laser welding (WL). Each group was divided in 4 subgroups, according to the size of the particles used in airborne particle abrasion A - Al2O3 (250 µm); B - Al2O3 (180 µm); C - Al2O3 (110 µm); D - Al2O3 (50 µm). Ceramic rings were fused around the CpTi rods. Specimens were invested and their tensile strength was measured at fracture with a universal testing machine at a crosshead speed of 2.0 mm/min and 200 kgf load cell. Statistical analysis was carried out with analysis of variance and compared using the independent t test (p<0.05).

RESULTS:

Significant differences were found among all subgroups (p<0.05). The highest and the lowest bond strength means were recorded in subgroups WLC (52.62 MPa) and LD (24.02 MPa), respectively.

CONCLUSION:

Airborne particle abrasion yielded significantly lower bond strength as the Al2O3 particle size decreased. Mechanical retention decreased in the laser-welded specimens, i.e. the metal-ceramic tensile bond strength was lower.
Asunto(s)


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Soldadura Dental / Titanio / Cerámica / Recubrimiento Dental Adhesivo / Abrasión Dental por Aire / Rayos Láser Idioma: Inglés Revista: J. appl. oral sci Asunto de la revista: Odontología Año: 2011 Tipo del documento: Artículo

Similares

MEDLINE

...
LILACS

LIS


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Soldadura Dental / Titanio / Cerámica / Recubrimiento Dental Adhesivo / Abrasión Dental por Aire / Rayos Láser Idioma: Inglés Revista: J. appl. oral sci Asunto de la revista: Odontología Año: 2011 Tipo del documento: Artículo