Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
Sampaio, Renata Kirita Doi; Wang, Linda; Carvalho, Rodrigo Varella de; Garcia, Eugenio José; Andrade, Andréa Mello de; Klein-Júnior, Celso Afonso; Grande, Rosa Helena Miranda; Moura, Sandra Kiss.
  • Sampaio, Renata Kirita Doi; University North of Paraná. Londrina. BR
  • Wang, Linda; University of São Paulo. Bauru School of Dentistry. Bauru. BR
  • Carvalho, Rodrigo Varella de; University North of Paraná. Londrina. BR
  • Garcia, Eugenio José; University of São Paulo. São Paulo. BR
  • Andrade, Andréa Mello de; University of São Paulo. São Paulo. BR
  • Klein-Júnior, Celso Afonso; Lutheran University of Brasil. Cachoeira do Sul. BR
  • Grande, Rosa Helena Miranda; University of São Paulo. São Paulo. BR
  • Moura, Sandra Kiss; University North of Paraná. Londrina. BR
J. appl. oral sci ; 21(1): 80-84, 2013. tab
Artículo en Inglés | LILACS, BBO | ID: lil-685000
ABSTRACT

Objectives:

This study aimed to compare the micro-tensile bond strength of methacrylate resin systems to a silorane-based restorative system on dentin after 24 hours and six months water storage. Material and

Methods:

The restorative systems Adper Single Bond 2/Filtek Z350 (ASB), Clearfil SE Bond/Z350 (CF), Adper SE Plus/Z350 (ASEP) and P90 Adhesive System/Filtek P90 (P90) were applied on flat dentin surfaces of 20 third molars (n=5). The restored teeth were sectioned perpendicularly to the bonding interface to obtain sticks (0.8 mm2) to be tested after 24 hours (24 h) and 6 months (6 m) of water storage, in a universal testing machine at 0.5 mm/min. The data was analyzed via two-way Analysis of Variance/Bonferroni post hoc tests at 5% global significance.

Results:

Overall outcomes did not indicate a statistical difference for the resin systems (p=0.26) nor time (p=0.62). No interaction between material × time was detected (p=0.28). Mean standard-deviation in MPa at 24 h and 6 m were ASB 31.38 (4.53) and 30.06 (1.95), CF 34.26 (3.47) and 32.75 (4.18), ASEP 29.54 (4.14) and 33.47 (2.47), P90 30.27 (2.03) and 31.34 (2.19).

Conclusions:

The silorane-based system showed a similar performance to methacrylate-based materials on dentin. All systems were stable in terms of bond strength up to 6 month of water storage.
Asunto(s)


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Recubrimientos Dentinarios / Dentina / Metacrilatos Límite: Humanos Idioma: Inglés Revista: J. appl. oral sci Asunto de la revista: Odontología Año: 2013 Tipo del documento: Artículo País de afiliación: Brasil Institución/País de afiliación: Lutheran University of Brasil/BR / University North of Paraná/BR / University of São Paulo/BR

Similares

MEDLINE

...
LILACS

LIS


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Recubrimientos Dentinarios / Dentina / Metacrilatos Límite: Humanos Idioma: Inglés Revista: J. appl. oral sci Asunto de la revista: Odontología Año: 2013 Tipo del documento: Artículo País de afiliación: Brasil Institución/País de afiliación: Lutheran University of Brasil/BR / University North of Paraná/BR / University of São Paulo/BR