Your browser doesn't support javascript.
loading
Strength of 3Y-TZP and feldspathic porcelain subjected to different cooling methods
Almeida-Júnior, Antonio Alves de; Longhini, Diogo; Galvão, Beatriz Regalado; Santos, Claudinei dos; Adabo, Gelson Luis.
  • Almeida-Júnior, Antonio Alves de; Universidade Tiradentes. School of Dentistry. Department of Oral Rehabilitation. Aracaju. BR
  • Longhini, Diogo; Universidade Estadual Paulista. School of Dentistry. Department of Dental Materials and Prosthodontics. Araraquara. BR
  • Galvão, Beatriz Regalado; Universidade Potiguar. School of Dentistry. Department of Oral Rehabilitation. Natal. BR
  • Santos, Claudinei dos; Universidade do Estado do Rio de Janeiro. Resende School of Technology. Department of engineering Materials. Resende. BR
  • Adabo, Gelson Luis; Universidade Estadual Paulista. School of Dentistry. Department of Dental Materials and Prosthodontics. Araraquara. BR
Braz. j. oral sci ; 13(2): 124-128, Apr-Jun/2014. tab, graf
Artículo en Inglés | LILACS | ID: lil-715609
ABSTRACT

AIM:

To investigate the effect of the cooling rate on flexural strength of monolayer and bilayer porcelain/zirconia (Y-TZP) bars.

METHODS:

Forty-five specimens were made for each design group (PM) monolithic specimens of veneer porcelain Vita VM9 (Vita, Germany); (ZM) monolithic specimens of zirconia (ZiHP; ProtMat, Brazil); (PB) bilayer specimens zirconia/porcelain with porcelain on lower surface; and (ZB) bilayer specimens porcelain/zirconia with zirconia on lower surface. Each group was cooled by three different methods after porcelain sintering slow specimens were cooled inside the turned-off furnace; normal specimens were removed from the furnace and cooled in air at room temperature; and fast specimens were removed from the furnace at 910°C and cooled by compressed air for 10 s. Specimens were polished and flexural strength was measured in water at 37 °C (n=15). Maximum load at fracture was recorded, and equations for simple (monolayer) and composite (bilayer) structures were used to calculate the flexural strength. RESULTS were analyzed using one-way ANOVA (p<0.05) and Tukey test separately for each design.

RESULTS:

The results of one-way ANOVA were statistically significant only for the PB group. The post-hoc Tukey test showed the highest flexural strength for fast cooling and the lowest for slow cooling; the normal cooling was statistically similar to both.

CONCLUSIONS:

Cooling methods affected only the flexural strength of bilayer specimens with porcelain on low surface (under tension) when the slow cooling method was used...
Asunto(s)


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Circonio / Porcelana Dental / Ciencia de los Materiales Idioma: Inglés Revista: Braz. j. oral sci Asunto de la revista: Odontología Año: 2014 Tipo del documento: Artículo / Documento de proyecto País de afiliación: Brasil Institución/País de afiliación: Universidade Estadual Paulista/BR / Universidade Potiguar/BR / Universidade Tiradentes/BR / Universidade do Estado do Rio de Janeiro/BR

Similares

MEDLINE

...
LILACS

LIS


Texto completo: Disponible Índice: LILACS (Américas) Asunto principal: Circonio / Porcelana Dental / Ciencia de los Materiales Idioma: Inglés Revista: Braz. j. oral sci Asunto de la revista: Odontología Año: 2014 Tipo del documento: Artículo / Documento de proyecto País de afiliación: Brasil Institución/País de afiliación: Universidade Estadual Paulista/BR / Universidade Potiguar/BR / Universidade Tiradentes/BR / Universidade do Estado do Rio de Janeiro/BR