Your browser doesn't support javascript.
loading
Protective effect of experimental mouthrinses containing NaF and TiF4 on dentin erosive loss in vitro
CASTILHO, Aline Rogéria Freire de; SALOMÃO, Priscila Maria Aranda; BUZALAF, Marília Afonso Rabelo; MAGALHÃES, Ana Carolina.
Afiliación
  • CASTILHO, Aline Rogéria Freire de; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Ciências Fisiológicas. Campinas. BR
  • SALOMÃO, Priscila Maria Aranda; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Ciências Fisiológicas. Campinas. BR
  • BUZALAF, Marília Afonso Rabelo; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Ciências Fisiológicas. Campinas. BR
  • MAGALHÃES, Ana Carolina; Universidade Estadual de Campinas. Faculdade de Odontologia de Piracicaba. Departamento de Ciências Fisiológicas. Campinas. BR
J. appl. oral sci ; J. appl. oral sci;23(5): 486-490, Sept.-Oct. 2015. tab
Article en En | LILACS, BBO | ID: lil-764153
Biblioteca responsable: BR1.1
ABSTRACT
Objective This in vitro study assessed the anti-erosive effect of experimental mouthrinses containing TiF4 and NaF on dentin erosive loss.Material and Methods Bovine dentin specimens were randomly allocated into the groups (n=15) 1) SnCl2/NaF/AmF (Erosion Protection®/GABA, pH 4.5, positive control); 2) experimental solution with 0.0815% TiF4(pH 2.5); 3) 0.105% NaF (pH 4.5); 4) 0.042% NaF+0.049% TiF4 (pH 4.4); 5) 0.063% NaF+0.036% TiF4 (pH 4.5); 6) no treatment (negative control). Each specimen was cyclically demineralized (Sprite Zero, pH 2.6, 4x90 s/day) and exposed to artificial saliva between the erosive challenges for 7 days. The treatment with the fluoride solutions was done 2x60 s/day, immediately after the first and the last erosive challenges of the day. Dentin erosive loss was measured by profilometry (μm). The data were analyzed using Kruskal Wallis/Dunn tests (p<0.05).Results Mouthrinses containing TiF4or Sn/F were able to show some protective effect against dentin erosive loss compared to negative control. The best anti-erosive effect was found for experimental solution containing 0.0815% TiF4 (100% reduction in dentin loss), followed by 0.042% NaF+0.049% TiF4 (58.3%), SnCl2/NaF/AmF (52%) and 0.063% NaF+0.036% TiF4 (40%). NaF solution (13.3%) did not significantly differ from control.Conclusion The daily application of experimental mouthrinse containing TiF4and NaF has the ability to reduce dentin erosion, as well as Erosion Protection® and TiF4 alone.
Asunto(s)
Palabras clave

Texto completo: 1 Índice: LILACS Asunto principal: Fluoruro de Sodio / Titanio / Erosión de los Dientes / Cariostáticos / Dentina / Fluoruros / Antisépticos Bucales Tipo de estudio: Evaluation_studies Límite: Animals Idioma: En Revista: J. appl. oral sci Asunto de la revista: ODONTOLOGIA Año: 2015 Tipo del documento: Article

Texto completo: 1 Índice: LILACS Asunto principal: Fluoruro de Sodio / Titanio / Erosión de los Dientes / Cariostáticos / Dentina / Fluoruros / Antisépticos Bucales Tipo de estudio: Evaluation_studies Límite: Animals Idioma: En Revista: J. appl. oral sci Asunto de la revista: ODONTOLOGIA Año: 2015 Tipo del documento: Article