ABSTRACT
<p><b>OBJECTIVE</b>To evaluate the marginal microleakage of porcelain-fused-to-metal crown using four different cements.</p><p><b>METHODS</b>Sixteen porcelain-fused-to-metal crowns were built and randomly divided into 4 group, luted onto standard prepared human forward molars using four different cements (glass ionomer cement, resin-modified glass ionomer cement, PanaviaF, Super-Bond C&B adhesive luting system). After temperature cycling test, all the crowns were then submerged in 2% fuchsin for 24 h. The marginal microleakage at tooth cement interfaces was observed using light stereomicroscopy and evaluated in classification index. The marginal microleakage grade of 4 groups were analyzed by SPSS 13.0.</p><p><b>RESULTS</b>The PanaviaF demonstrated the least marginal microleakage, Super-Bond C&B adhesive luting system, resin-modified glass ionomer cement showed an intermediate level of marginal microleakage, glass ionomer cement was associated with severe marginal microleakage (total, Chi2 = 157.60, P < 0.01; among the different groups, P<0.05).</p><p><b>CONCLUSION</b>Adhesive resin luting system which is the first selection in clinical is better than glass ionomer cement and is good at porcelain-fused-to-metal crown.</p>
Texto completo:
1
Índice:
WPRIM
Asunto principal:
Compuestos de Boro
/
Cementación
/
Adaptación Marginal Dental
/
Cementos de Resina
/
Coronas
/
Cementos Dentales
/
Filtración Dental
/
Porcelana Dental
/
Cementos de Ionómero Vítreo
/
Metales
Límite:
Humans
Idioma:
Zh
Revista:
West China Journal of Stomatology
Año:
2011
Tipo del documento:
Article