Microtensile bonding strength between root canal wall and root canal rehabilitation materials / 实用口腔医学杂志
Journal of Practical Stomatology
;
(6)1995.
Artículo
en Chino
| WPRIM
| ID: wpr-670747
ABSTRACT
Objective:
To test the microtensile bonding strength between root canal wall and Bis-Core, and that between root canal wall and Chemil Superior glass-ionomer.Methods:
10 human maxillary incisors extracted within one week were kept for another one week after root canal treatment and removeal of the crowns,each root was splited into two parts along with the long axis by Isomet saw, the bonding interface on one third of upside of root dentin smear layer was made with Diamond bur at a high-speed. Then Bis-Core and Chemil Superior glass-ionomer were put on root canal inner surface of each half part of the root respectively, samples with the size of 1.00 mm?1.00 mm were prepared by Isomet saw. Two samples in which bonding interface was perpendiculur to load were selected and fixed in Microtensile testing machine for bonding strength test.Results:
Microtensile bonding strength(MPa) between Bis-Core and root canal inner wall and that between root canal inner wall and Chemil Superior glass-ionomer was 20.65?1.72 and 12.89?1.63 respectively(P
Texto completo:
Disponible
Índice:
WPRIM (Pacífico Occidental)
Idioma:
Chino
Revista:
Journal of Practical Stomatology
Año:
1995
Tipo del documento:
Artículo
Similares
MEDLINE
...
LILACS
LIS