RESUMEN
RESUMEN Los laminados vitrocerámicos ultradelgados constituyen una alternativa conservadora para la resolución de alteraciones estéticas. Sin embargo, su acondicionamiento con ácido fluorhídrico suele no estar exento de complicaciones, por lo que el uso de un sistema autograbante en base a polifluoruro de amonio (Monobond Etch&Prime, MEP) permite disminuir el riesgo de sobregrabado, simplificando la técnica. El presente reporte presenta el seguimiento a dieciocho meses de un caso clínico resuelto mediante laminados vitrocerámicos acondicionados únicamente con MEP. Caso. Paciente joven con alteraciones estéticas en el sector anterosuperior. Se realizaron preparaciones conservadoras para la confección de laminados ultradelgados en disilicato de litio (e.maxPress). Las vitrocerámicas fueron acondicionadas sólo con MEP y se cementaron con Variolink Esthetic LC. Al año y medio las restauraciones se observaron indemnes, manteniendo un buen ajuste marginal y ausencia de tinciones. Conclusiones. MEP aparece como una alternativa prometedora para reemplazar al ácido fluorhídrico en la cementación de laminados vitrocerámicos.
ABSTRACT
ABSTRACT Ultrathin glass-ceramic veneers are a conservative approach for the restorative treatment of aesthetic disorders in the anterior region. However, surface conditioning with hydrofluoric acid of the thin structures can be usually a challenging step. Therefore, the use of a self-etching ceramic primer containing ammonium polyfluoride (Monobond Etch&Prime, MEP) offers a simplified technique with a reduced risk of overetching. Here we present an 18-month follow-up of ultrathin glass-ceramic veneers conditioned with MEP only. Case. Young female patient with an aesthetic disorder in the front region. The four upper incisors were conservatively prepared for ultrathin lithium disilicate (e.maxPress) veneers. Pre-treatment of the glass-ceramics consisted only of MEP application, followed by adhesive cementation with Variolink Esthetic LC. At the 1.5-year recall, the restorations appeared undamaged, with no marginal gap or staining. Conclusions. MEP constitutes a promising alternative to hydrofluoric acid for the adhesive cementation of glass-ceramic veneers.
Mots clés
Texte intégral:
1
Indice:
LILACS
Sujet Principal:
Ciments dentaires
/
Facettes dentaires
/
Mordançage
Limites du sujet:
Adult
/
Female
/
Humans
langue:
Es
Texte intégral:
Int. j interdiscip. dent. (Print)
Thème du journal:
Medicina Cl¡nica
/
Odontologia
/
Patologia
Année:
2021
Type:
Article