The Effect of Restoration Polymerization and Residual Dentine Thickness on Thermal Changes of Pulp Chamber of Immature Permanent Teeth
Kolçakoğlu, Kevser; Aksoy, Merve; Bal, Cenkhan; Demirel, Akif; Öz, Firdevs Tulga.
Affiliation
  • Kolçakoğlu, Kevser; Erciyes University. Faculty of Dentistry. Department of Pedodontics. Kayseri. TR
  • Aksoy, Merve; University of Health Sciences. Gulhane Faculty of Dentistry. Department of Pedodontics. Ankara. TR
  • Bal, Cenkhan; University of Health Sciences. Gulhane Faculty of Dentistry. Department of Pedodontics. Ankara. TR
  • Demirel, Akif; Ankara University. Faculty of Dentistry. Department of Pedodontics. Ankara. TR
  • Öz, Firdevs Tulga; Ankara University. Faculty of Dentistry. Department of Pedodontics. Ankara. TR
Pesqui. bras. odontopediatria clín. integr ; 24: e230179, 2024. tab, graf
Article de En | LILACS, BBO | ID: biblio-1564868
Bibliothèque responsable: BR1264.1
Localisation: 1519-0501-pboci-24-e230179.xml
ABSTRACT
ABSTRACT

Objective:

To evaluate the pulpal temperature changes due to the polymerisation of resin and glass ionomer-based materials in dentine thicknesses in immature permanent teeth with open apices. Material and

Methods:

Forty extracted sound human third molar teeth with open apices were included. The width of the cavities prepared on the occlusal surface was 4×5 mm. The depth was 2 mm in the resin groups. 4 mm in the groups in which glass ionomer liner was applied before composite restoration. The coronal parts of the samples were then placed on an acrylic plate with three gaps for feeding-extraction needles and the thermocouple. The temperature changes were recorded. The data was analyzed by SPSS. Statistical significance was accepted as p<0.05.

Results:

The temperature increase in the group of 1 mm remaining dentin thickness revealed higher results than the values detected from the 2 mm group (1.01 °C) (p=0.00). The mean values (1.49 °C, 1mm) of temperature changes in only glass ionomer applied group were lower than the avarage values (2.210°C, 1mm) determined in the polymerization process of resin composites with light-emitting diode devices.

Conclusion:

In a remaining dentin thickness of 1 mm in teeth with open apices, using a glass ionomer liner might be a useful effort for protecting the pulp from the heat generated by polymerisation devices.
Sujet(s)
Mots clés

Texte intégral: 1 Indice: LILACS Sujet Principal: Résines composites / Denture permanente / Apex de la racine de la dent / Test pulpaire / Ciment ionomère au verre Limites du sujet: Humans langue: En Texte intégral: Pesqui. bras. odontopediatria clín. integr Thème du journal: ODONTOLOGIA Année: 2024 Type: Article

Texte intégral: 1 Indice: LILACS Sujet Principal: Résines composites / Denture permanente / Apex de la racine de la dent / Test pulpaire / Ciment ionomère au verre Limites du sujet: Humans langue: En Texte intégral: Pesqui. bras. odontopediatria clín. integr Thème du journal: ODONTOLOGIA Année: 2024 Type: Article