Roughness and porosity of provisional crowns
RPG rev. pos-grad
;
18(2): 108-112, abr.-jun. 2011. ilus, graf
Article
Dans Anglais
| LILACS
| ID: lil-679849
RESUMO
This study aimed at evaluating the surface roughness and porosity of an acrylic resin used for provisional crowns. Six different processing techniques (direct and indirect) were assessed (I) heat-cured acrylic resin under pressure; (II) heat-aided autopolymerizing resin under pressure; (III) autopolymerizing resin under pressure; (IV) bead-brush technique; (V) autopolymerizing resin in sandy stage; (VI) autopolymerizing resin in plastic stage. Twelve specimens were made for each test group. Roughness was evaluated with a rugosimeter, and porequantification was performed using a stereoscopic magnifying lens. The highest mean surface roughness (Ra = 0.908 mm) was measured for Group VI. The lowest surface roughness value (Ra = 0.141 mm) was determined for Group I. Significant differences in mean surface roughness were found between direct and indirect techniques. Direct techniques reached the highest roughness and porosity values; its use should be restricted to avoid creating favorable conditions for microorganism proliferation
Recherche sur Google
Indice:
LILAS (Amériques)
Sujet Principal:
Orthodontie
/
Prothèses dentaires
/
Couronne dentaire
/
Restaurations dentaires temporaires
/
Odontologie
langue:
Anglais
Texte intégral:
RPG rev. pos-grad
Année:
2011
Type:
Article
Pays d'affiliation:
Brésil
Institution/Pays d'affiliation:
Universidade Federal de Alfenas/BR
/
Universidade de São Paulo/BR
Documents relatifs à ce sujet
MEDLINE
...
LILACS
LIS