Microstructural and mechanical analysis of two CAD-CAM lithium disilicate glass-reinforced ceramics
Tavares, Lucas do Nascimento; Zancopé, Karla; Silva, Anielle Christine Almeida; Raposo, Luís Henrique Araújo; Soares, Carlos José; Neves, Flávio Domingues das.
  • Tavares, Lucas do Nascimento; Universidade Federal de Uberlândia. School of Dentistry. Department of Occlusion, Fixed Prosthesis and Dental Materials. Uberlândia. BR
  • Zancopé, Karla; Universidade Federal de Uberlândia. School of Dentistry. Department of Occlusion, Fixed Prosthesis and Dental Materials. Uberlândia. BR
  • Silva, Anielle Christine Almeida; Universidade Federal de Uberlândia. Physics Institute. Laboratory of New Insulating and Semiconductor Materials. Uberlândia. BR
  • Raposo, Luís Henrique Araújo; Universidade Federal de Uberlândia. School of Dentistry. Department of Occlusion, Fixed Prosthesis and Dental Materials. Uberlândia. BR
  • Soares, Carlos José; Universidade Federal de Uberlândia. School of Dentistry. Department of Operative Dentistry and Dental Materials. Uberlândia. BR
  • Neves, Flávio Domingues das; Universidade Federal de Uberlândia. School of Dentistry. Department of Occlusion, Fixed Prosthesis and Dental Materials. Uberlândia. BR
Braz. oral res. (Online) ; 34: e004, 2020. tab, graf
Artigo em Inglês | LILACS | ID: biblio-1055523
ABSTRACT
Abstract The aim of this study was to analyze the structural, morphological and mechanical properties of two different lithium disilicate glass-reinforced ceramics for CAD-CAM systems (IPS e.max CAD and Rosetta SM). Five methodologies were used for both ceramics: microstructure (n = 2) was analyzed using x-ray diffraction (XRD); morphological properties (n = 2) were analyzed by scanning electron microscopy (SEM), with and without hydrofluoric etching; porosity (n = 3) was assessed using 3D micro-computed tomography (micro-CT); flexural strength was measured (n =1 0) using the three-point bending test; and bond strength was determined with self-adhesive resin cement (n = 10), using a microshear bond test. After performing all the tests, the data were analyzed using t-Student test and two-way ANOVA. All the tests used a significance level of α = 0.05. High peak positions corresponding to standard lithium metasilicate and lithium disilicate with similar intensities were observed for both ceramics in the XRD analysis. Morphological analysis showed that the crystalline structure of the two ceramics studied showed no statistical difference after acid etching. Additionally, no significant differences were recorded in the number or size of the pores for the ceramics evaluated. Moreover, no differences in flexural strength were found for the ceramic materials tested, or in the bond strength to ceramic substrates for the resin cements. Based on the study results, no significant differences were found between the two CAD-CAM lithium disilicate glass-reinforced ceramics tested, since they presented similar crystalline structures with comparable intensities, and similar total porosity, flexural strength and bond strength.
Assuntos


Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Cerâmica / Desenho Assistido por Computador / Porcelana Dentária / Vidro Tipo de estudo: Estudos de avaliação Idioma: Inglês Revista: Braz. oral res. (Online) Assunto da revista: Odontologia Ano de publicação: 2020 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Universidade Federal de Uberlândia/BR

Similares

MEDLINE

...
LILACS

LIS


Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Cerâmica / Desenho Assistido por Computador / Porcelana Dentária / Vidro Tipo de estudo: Estudos de avaliação Idioma: Inglês Revista: Braz. oral res. (Online) Assunto da revista: Odontologia Ano de publicação: 2020 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Universidade Federal de Uberlândia/BR