Your browser doesn't support javascript.
loading
One-year aging effects on microtensile bond strengths of composite and repairs with different surface treatments
SOUZA, Marcela Oliveira de; LEITUNE, Vicente Castelo Branco; RODRIGUES, Stéfani Becker; SAMUEL, Susana Maria Werner; COLLARES, Fabrício Mezzomo.
  • SOUZA, Marcela Oliveira de; Universidade Federal do Rio Grande do Sul. School of Dentistry. Dental Materials Laboratory. Porto Alegre. BR
  • LEITUNE, Vicente Castelo Branco; Universidade Federal do Rio Grande do Sul. School of Dentistry. Dental Materials Laboratory. Porto Alegre. BR
  • RODRIGUES, Stéfani Becker; Universidade Federal do Rio Grande do Sul. School of Dentistry. Dental Materials Laboratory. Porto Alegre. BR
  • SAMUEL, Susana Maria Werner; Universidade Federal do Rio Grande do Sul. School of Dentistry. Dental Materials Laboratory. Porto Alegre. BR
  • COLLARES, Fabrício Mezzomo; Universidade Federal do Rio Grande do Sul. School of Dentistry. Dental Materials Laboratory. Porto Alegre. BR
Braz. oral res. (Online) ; 31: e4, 2017. tab, graf
Artigo em Inglês | LILACS | ID: biblio-839528
ABSTRACT
Abstract The present study aimed to evaluate effects of different surface treatments and aging of composite cylinders on bond strength of composite resin repair. Thirty-two composite cylinders were produced and divided into four groups according to type of surface treatment and storage time of composite cylinder and repair. Cylinder surface of control group (Gcontrol) received no treatment before composite repair. Other groups were sandblasted with aluminum oxide (GAl2O3), followed by silane (GAl2O3sil) or adhesive (GAl2O3ad). Composite cylinders were stored in artificial saliva for either 24 hours or 1 year. Repairs were performed and stored in artificial saliva for 24 hours or 1 year and repair strength was evaluated using microtensile bond strength test. Data were submitted to Student’s t test, two-way ANOVA, and post hoc test for storage time and treatment (α = 0.05). Gcontrol group showed lower values of aging of composite cylinder and storage time of repair (24 hours or 1 year for both) compared with other groups (p < 0.05). GAl2O3ad and GAl2O3sil groups did not exhibit decreased microtensile bond strength with aged repairs (1 year; p > 0.05). Polymer degradation was significant for composite cylinders during the first year of storage in Gcontrol, GAl2O3, and GAl2O3ad groups (p < 0.05). In GAl2O3sil group, storage time of composite cylinders was not significant (p > 0.05). Aging of composite resin influenced bond strength of restoration repair for up to 1 year. Sandblasting with Al2O3, followed by application of silane layer, produced high bond strength after composite or repair aging.
Assuntos


Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Resistência à Tração / Colagem Dentária / Resinas Compostas / Cimentos de Resina / Reparação de Restauração Dentária Tipo de estudo: Estudos de avaliação Idioma: Inglês Revista: Braz. oral res. (Online) Assunto da revista: Odontologia Ano de publicação: 2017 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Universidade Federal do Rio Grande do Sul/BR

Similares

MEDLINE

...
LILACS

LIS


Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Resistência à Tração / Colagem Dentária / Resinas Compostas / Cimentos de Resina / Reparação de Restauração Dentária Tipo de estudo: Estudos de avaliação Idioma: Inglês Revista: Braz. oral res. (Online) Assunto da revista: Odontologia Ano de publicação: 2017 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Universidade Federal do Rio Grande do Sul/BR