Correlation between metal-ceramic bond strength and coefficient of linear thermal expansion difference
Lopes, Stella Crosara; Pagnano, Valéria Oliveira; Rollo, João Manuel Domingos de Almeida; Leal, Mônica Barbosa; Bezzon, Osvaldo Luiz.
  • Lopes, Stella Crosara; University of São Paulo. Dental School of Ribeirão Preto. Department of Dental Materials and Prosthodontics. Ribeirão Preto. BR
  • Pagnano, Valéria Oliveira; University of São Paulo. Dental School of Ribeirão Preto. Dental Materials and Prosthodontics. Ribeirão Preto. BR
  • Rollo, João Manuel Domingos de Almeida; University of São Paulo. Engineering School of São Carlos. São Carlos. BR
  • Leal, Mônica Barbosa; University of São Paulo. Dental School of Ribeirão Preto. Department of Dental Materials and Prosthodontics. Ribeirão Preto. BR
  • Bezzon, Osvaldo Luiz; University of São Paulo. Dental School of Ribeirão Preto. Dental Materials and Prosthodontics. Ribeirão Preto. BR
J. appl. oral sci ; 17(2): 122-128, Mar.-Apr. 2009. ilus, graf, tab
Artigo em Inglês | LILACS | ID: lil-503990
ABSTRACT
The purpose of this study was to evaluate the metal-ceramic bond strength (MCBS) of 6 metal-ceramic pairs (2 Ni-Cr alloys and 1 Pd-Ag alloy with 2 dental ceramics) and correlate the MCBS values with the differences between the coefficients of linear thermal expansion (CTEs) of the metals and ceramics. Verabond (VB) Ni-Cr-Be alloy, Verabond II (VB2), Ni-Cr alloy, Pors-on 4 (P), Pd-Ag alloy, and IPS (I) and Duceram (D) ceramics were used for the MCBS test and dilatometric test. Forty-eight ceramic rings were built around metallic rods (3.0 mm in diameter and 70.0 mm in length) made from the evaluated alloys. The rods were subsequently embedded in gypsum cast in order to perform a tensile load test, which enabled calculating the CMBS. Five specimens (2.0 mm in diameter and 12.0 mm in length) of each material were made for the dilatometric test. The chromel-alumel thermocouple required for the test was welded into the metal test specimens and inserted into the ceramics. ANOVA and Tukey's test revealed significant differences (p=0.01) for the MCBS test results (MPa), with PI showing higher MCBS (67.72) than the other pairs, which did not present any significant differences. The CTE (10-6 oC-1) differences were VBI (0.54), VBD (1.33), VB2I (-0.14), VB2D (0.63), PI (1.84) and PD (2.62). Pearson's correlation test (r=0.17) was performed to evaluate of correlation between MCBS and CTE differences. Within the limitations of this study and based on the obtained results, there was no correlation between MCBS and CTE differences for the evaluated metal-ceramic pairs.
Assuntos

Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Colagem Dentária / Ligas Metalo-Cerâmicas Tipo de estudo: Estudos de avaliação Idioma: Inglês Revista: J. appl. oral sci Assunto da revista: Odontologia Ano de publicação: 2009 Tipo de documento: Artigo / Documento de projeto País de afiliação: Brasil Instituição/País de afiliação: University of São Paulo/BR

Similares

MEDLINE

...
LILACS

LIS

Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Colagem Dentária / Ligas Metalo-Cerâmicas Tipo de estudo: Estudos de avaliação Idioma: Inglês Revista: J. appl. oral sci Assunto da revista: Odontologia Ano de publicação: 2009 Tipo de documento: Artigo / Documento de projeto País de afiliação: Brasil Instituição/País de afiliação: University of São Paulo/BR