The effect of repeated bracket recycling on the shear bond strength of different orthodontic adhesives
Lunardi, Nádia; Gameiro, Gustavo Hauber; Magnani, Maria Beatriz Borges de Araújo; Nouer, Darcy Flávio; Siqueira, Vânia Célia de; Consani, Simonides; Pereira-Neto, João Sarmento.
  • Lunardi, Nádia; s.af
  • Gameiro, Gustavo Hauber; University of Campinas. Piracicaba Dental School. Orthodontics Division. Department of Pediatric Dentistry. Piracicaba. BR
  • Magnani, Maria Beatriz Borges de Araújo; University of Campinas. Piracicaba Dental School. Orthodontics Division. Department of Pediatric Dentistry. Piracicaba. BR
  • Nouer, Darcy Flávio; University of Campinas. Piracicaba Dental School. Orthodontics Division. Department of Pediatric Dentistry. Piracicaba. BR
  • Siqueira, Vânia Célia de; University of Campinas. Piracicaba Dental School. Orthodontics Division. Department of Pediatric Dentistry. Piracicaba. BR
  • Consani, Simonides; University of Campinas. Piracicaba Dental School. Dental Materials Division. Department of Restorative Dentistry. Piracicaba. BR
  • Pereira-Neto, João Sarmento; University of Campinas. Piracicaba Dental School. Department of Pediatric Dentistry. Piracicaba. BR
Braz. j. oral sci ; 7(27): 1648-1652, Oct.-Dec. 2008. ilus, tab
Artigo em Inglês | LILACS, BBO | ID: lil-521333
ABSTRACT

Aim:

The aim of this study was to evaluate the effect of two consecutive recycling procedures on the shear bond strength of different orthodontic adhesives.

Methods:

Edgewise brackets were bonded to the buccal surfaces of 40 bovine incisors using the following bonding materials Concise (group I), Transbond XT (group II), Smart Bond (group III) and Fuji Ortho (group IV). The teeth were stored in water at 37°C for 24 h, thermocycled between 5 and 55°C, and debonded using an Instron machine at a crosshead speed of 0.5 mm/min. In all groups, the bonded brackets were detached and rebonded after recycling by 50-µm particle aluminum oxide blasting. After the second recording of retentive strengths, the recycling procedure, the rebonding and the shear bond strength test were repeated. Data were analyzed statistically by ANOVA and Tukey’s test at 5% significance level.

Results:

The results showed that repeated recycling did not interfere in retention of brackets, regardless of the adhesive used. The highest shear bond strength values were obtained after bonding with Transbond XT, independent of the recycling procedure.

Conclusion:

Repeated bracket recycling using 50-µm aluminum oxide particle air abrasion did not affect the shear bond strength of metallic brackets bonded with different orthodontic adhesives.
Assuntos

Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Colagem Dentária / Braquetes Ortodônticos / Abrasão Dental por Ar / Resistência ao Cisalhamento Limite: Animais Idioma: Inglês Revista: Braz. j. oral sci Assunto da revista: Odontologia Ano de publicação: 2008 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: University of Campinas/BR

Similares

MEDLINE

...
LILACS

LIS

Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Colagem Dentária / Braquetes Ortodônticos / Abrasão Dental por Ar / Resistência ao Cisalhamento Limite: Animais Idioma: Inglês Revista: Braz. j. oral sci Assunto da revista: Odontologia Ano de publicação: 2008 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: University of Campinas/BR