Comparative study of flexural strength and elasticity modulus in two types of direct fiber-reinforced systems
Gaspar Junior, Alfredo de Aquino; Lopes, Manuela Wanderley Ferreira; Gaspar, Gabriela da Silveira; Braz, Rodivan.
  • Gaspar Junior, Alfredo de Aquino; Federal University of Pernambuco. School of Dentistry. Department of Prosthodontics and Buco-facial Surgery. Recife. BR
  • Lopes, Manuela Wanderley Ferreira; Federal University of Pernambuco. School of Dentistry. Department of Prosthodontics and Buco-facial Surgery. Recife. BR
  • Gaspar, Gabriela da Silveira; University of Pernambuco. School of Dentistry. Department of Restorative Dentistry. Camaragibe. BR
  • Braz, Rodivan; University of Pernambuco. School of Dentistry. Department of Restorative Dentistry. Camaragibe. BR
Braz. oral res ; 23(3): 236-240, 2009. graf, tab
Artigo em Inglês | LILACS | ID: lil-530258
ABSTRACT
The objective of this study was to compare the flexural strength and elasticity modulus of two types of staple reinforcement fibers, Interlig - Ângelus®/glass (Londrina, PR, Brazil) and Connect - KerrLab®/polyethylene (MFG Co., West Collins Orange, CA, USA), which are widely used in Dentistry for chairside use, after varying the number of layers employed and submitting or not to thermocycling. This study was performed on 72 specimens, divided into 8 groups G1 - single layer of Interlig fibers without thermocycling; G2 - double layer of Interlig fibers without thermocycling; G3 - single layer of Interlig fibers with thermocycling; and G4 - double layer of Interlig fibers with thermocycling; G5 - single layer of Connect fibers without termocycling; G6 - double layer of Connect fibers without termocycling; G7 - single layer of Connect fibers with termocycling; G8 - double layer of Connect fibers with termocycling. For each group, values for flexural strength and elasticity modulus were obtained. The polyethylene fiber employed in a double layer presented the highest flexural strength (p < 0.05), independently of thermocycling (p < 0.001), when compared to the other evaluated combinations. The polyethylene fiber, used in a single layer without thermocycling, demonstrated a significantly higher elasticity modulus, when compared to the other groups (p < 0.05). Within the limits of this study, it was concluded that the polyethylene fiber in a double layer appears to be more resistant, regardless of whether it was submitted to thermocycling or not.
Assuntos

Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Resistência à Tração / Teste de Materiais / Resinas Compostas / Análise do Estresse Dentário Idioma: Inglês Revista: Braz. oral res Assunto da revista: Odontologia Ano de publicação: 2009 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Federal University of Pernambuco/BR

Similares

MEDLINE

...
LILACS

LIS

Texto completo: DisponíveL Índice: LILACS (Américas) Assunto principal: Resistência à Tração / Teste de Materiais / Resinas Compostas / Análise do Estresse Dentário Idioma: Inglês Revista: Braz. oral res Assunto da revista: Odontologia Ano de publicação: 2009 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Federal University of Pernambuco/BR