In in-vitro evaluation of effect of different finish lines on marginal adaptation in metal-ceramic restorations under thermo-mechanical loading.
Artigo em Inglês | IMSEAR | ID: sea-140085
ABSTRACT
The aim of this study was to evaluate the marginal gap in terms of cement film thickness associated with shoulder, shoulder with 45° bevel, shoulder with 30° bevel and chamfer, under thermo-mechanical loading. Forty human mandibular molars were prepared and restored with ceramo-metal crowns. Teeth were thermo-mechanically loaded and vertically sectioned to evaluate the cement film thickness. Shoulder with 45° bevel provided the least marginal gap as compared with all the tested finish lines.
Assuntos

Texto completo: DisponíveL Índice: IMSEAR (Sudeste Asiático) Assunto principal: Paládio / Prata / Estresse Mecânico / Propriedades de Superfície / Temperatura / Força de Mordida / Teste de Materiais / Humanos / Ligas Metalo-Cerâmicas / Adaptação Marginal Dentária Idioma: Inglês Ano de publicação: 2011 Tipo de documento: Artigo

Similares

MEDLINE

...
LILACS

LIS

Texto completo: DisponíveL Índice: IMSEAR (Sudeste Asiático) Assunto principal: Paládio / Prata / Estresse Mecânico / Propriedades de Superfície / Temperatura / Força de Mordida / Teste de Materiais / Humanos / Ligas Metalo-Cerâmicas / Adaptação Marginal Dentária Idioma: Inglês Ano de publicação: 2011 Tipo de documento: Artigo