STATEMENT OF PROBLEM:
There have been few studies about the marginal fit of Auro Galvano Crowns.PURPOSE:
The purpose of this study was to compare the marginal fit of the anterior single restorations. MATERIAL ANDMETHODS:
The in vitro marginal discrepancies of metal-ceramic, Auro Galvano Crown and coping were evaluated and compared. The Auro Gavano Crowns were made from one extracted maxillary central incisor prepared by milling machine. 30crowns per each system were fabricated. Measurements of a crown were recorded at 50 points that were randomly selected for marginal gap evaluation. Parametric statistical analysis was performed for the results.RESULTS:
Mean marginal gap dimensions and standard deviations at the marginal opening for the anterior single crowns were 74+/-21micrometer for the control (metal-ceramic restoration), 45+/-11 micrometer for Auro Galvano Crown coping, and 51+/-9 micrometer for the Auro Galvano Crown.CONCLUSIONS:
Auro Galvano Crown showed significantly smaller (P .05)
Texto completo:
DisponíveL
Índice:
WPRIM (Pacífico Ocidental)
Assunto principal:
Cerâmica
/
Coroas
/
Incisivo
Idioma:
Inglês
Revista:
The Journal of Korean Academy of Prosthodontics
Ano de publicação:
2004
Tipo de documento:
Artigo
Similares
MEDLINE
...
LILACS
LIS