Opt Express ; 32(4): 5729-5736, 2024 Feb 12.
Article in English | MEDLINE | ID: mdl-38439291

ABSTRACT

Monolayers containing subnanometer striations of silica and hafnia to form composite materials at varying ratios are explored as a method to develop high-index dielectric layers with increased laser-induced-damage thresholds (LIDTs). These layers can then be used in multilayer dielectric coatings for short-pulse, high-peak-power laser applications, particularly in regions of the highest electric-field intensity. Fabrication is achieved by means of exposure to two different evaporant vapor plumes, where local exposure to each plume is controlled via shielding to prevent simultaneous exposure. The LIDT of the resulting layers has been evaluated at 1053 nm with 600-fs pulses. The results indicate that such hafnia/silica layers exhibit LIDTs similar to silica for a refractive index of ≤1.65. These results suggest that the use of these layers in locations subjected to high electric-field intensity within multilayer dielectric coatings may significantly improve the LIDT, with this deposition process providing particular benefit for scaling to large-aperture, high-fluence components.

2.
Sci Rep ; 13(1): 6524, 2023 Apr 21.
Article in English | MEDLINE | ID: mdl-37085662

ABSTRACT

Potassium dihydrogen phosphate (KDP) and its deuterated analog (DKDP) are unique nonlinear optical materials for high power laser systems. They are used widely for frequency conversion and polarization control by virtue of the ability to grow optical-quality crystals at apertures suitable for fusion-class laser systems. Existing methods for freeform figuring of KDP/DKDP optics do not produce surfaces with sufficient laser-induced-damage thresholds (LIDT's) for operation in the ultraviolet portion of high-peak-power laser systems. In this work, we investigate fluid jet polishing (FJP) using a nonaqueous slurry as a sub-aperture finishing method for producing freeform KDP surfaces. This method was used to selectively polish surface areas to different depths on the same substrate with removals ranging from 0.16 µm to 5.13 µm. The finished surfaces demonstrated a slight increase in roughness as the removal depth increased along with a small number of fracture pits. Laser damage testing with 351 nm, 1 ns pulses demonstrated excellent surface damage thresholds, with the highest values in areas devoid of fracture pits. This work demonstrates, for the first time, a method that enables fabrication of a waveplate that provides tailored polarization randomization that can be scaled to meter-sized optics. Furthermore, this method is based on FJP technology that incorporates a nonaqueous slurry specially designed for use with KDP. This novel nonaqueous FJP process can be also used for figuring other types of materials that exhibit similar challenging inherent properties such as softness, brittleness, water-solubility, and temperature sensitivity.

3.
Sci Rep ; 12(1): 10969, 2022 Jun 29.
Article in English | MEDLINE | ID: mdl-35768616

ABSTRACT

Interactions of liquid crystals (LC's) with polarized light have been studied widely and have spawned numerous device applications, including the fabrication of optical elements for high-power and large-aperture laser systems. Currently, little is known about both the effect of incident polarization state on laser-induced-damage threshold (LIDT) and laser-induced functional threshold (LIFT) behavior at sub-LIDT fluences under multipulse irradiation conditions. This work reports on the first study of the nanosecond-pulsed LIDT's dependence on incident polarization for several optical devices employing oriented nematic and chiral-nematic LC's oriented by surface alignment layers. Accelerated lifetime testing was also performed to characterize the ability of these devices to maintain their functional performance under multipulse irradiation as a function of the laser fluence at both 1053 nm and 351 nm. Results show that the LIDT varies as a function of input polarization by 30-80% within the same device, while the multipulse LIFT (which can differ from the nominal LIDT) depends on irradiation conditions such as laser fluence and wavelength.

4.
Opt Lett ; 43(15): 3702-3705, 2018 Aug 01.
Article in English | MEDLINE | ID: mdl-30067659

ABSTRACT

Femtosecond laser-induced damage and ablation (fs-LIDA) is a rich field in extreme non-perturbative nonlinear optics with wide ranging applications, including laser micro- and nano-machining, waveguide writing, and eye surgery. Our understanding of fs-LIDA, however, is limited mostly to visible and near-infrared wavelengths. In this work, we systematically study single-shot, fs-laser ablation (fs-LIA) of single-crystal germanium from near- to mid-infrared wavelengths, and compare the fs-LIA wavelength scaling with two widely used models. We show that these models are inadequate, particularly at mid-infrared wavelengths. Instead, a hybrid model is proposed involving Keldysh ionization rates, a constant free-carrier density threshold, and multi-band effects, which yields good agreement with experimental observations. Aspects of this model may be applied to understanding other strong-field non-perturbative phenomena in solids.

5.
Opt Express ; 24(25): 28858-28868, 2016 Dec 12.
Article in English | MEDLINE | ID: mdl-27958528

ABSTRACT

A systematic study of few-cycle pulse laser induced damage threshold (LIDT) determination was performed for commercially-available ultra-broadband optics, (i.e. chirped mirrors, silver mirrors, beamsplitters, etc.) in vacuum and in air, for single and multi-pulse regime (S-on-1). Multi-pulse damage morphology at fluences below the single-pulse LIDT was studied in order to investigate the mechanisms leading to the onset of damage. Stark morphological contrast was observed between multi-pulse damage sites formed in air versus those in vacuum. One effect of vacuum testing compared to air included suppression of laser-induced periodic surface structures (LIPSS) formation, possibly influenced by a reduced presence of damage debris. Another effect of vacuum was occasional lowering of LIDT, which appears to be due to the stress-strain performance of the coating design during laser irradiation and under the external stress of vacuum ambience. A fused silica substrate is also examined, and a non-LIPSS nanostructuring is observed on the surface. Possible mechanisms are discussed.

6.
Opt Express ; 23(15): 19522-34, 2015 Jul 27.
Article in English | MEDLINE | ID: mdl-26367610

ABSTRACT

Laser induced periodic surface structures (LIPSS or ripples) were generated on single crystal germanium after irradiation with multiple 3 µm femtosecond laser pulses at a 45° angle of incidence. High and low spatial frequency LIPSS (HSFL and LSFL, respectively) were observed for both s- and p-polarized light. The measured LSFL period for p-polarized light was consistent with the currently established LIPSS origination model of coupling between surface plasmon polaritons (SPP) and the incident laser pulses. A vector model of SPP coupling is introduced to explain the formation of s-polarized LSFL away from the center of the damage spot. Additionally, a new method is proposed to determine the SPP propagation length from the decay in ripple depth. This is used along with the measured LSFL period to estimate the average electron density and Drude collision time of the laser-excited surface. Finally, full-wave electromagnetic simulations are used to corroborate these results while simultaneously offering insight into the nature of LSFL formation.