1.
J Environ Manage ; 306: 114375, 2022 Mar 15.
Article in English | MEDLINE | ID: mdl-35051819

ABSTRACT

Some unit operations in wastewater treatment plants (WWTPs), such as settling tanks and pipes for aeration or sludge transfer, are composed of austenitic stainless steel (EN 1.4307 or EN 1.4404) instead of galvanised or painted carbon steel to reduce the maintenance costs. The sensitivity to pitting and crevice corrosion of austenitic grades in certain WWTP environments has also led to the use of duplex grades. The purpose of this study is to evaluate the maintenance of piping systems (WWTPs) and its effect on their life cycle environmental impacts and costs (LCC) for both austenitic and duplex stainless steel grades. The final objective is to aid grade selection for piping in a WWTP environment. The considered functional unit (FU) is a complete piping system. Conventional austenitic stainless steel grades (e.g., EN 1.4404) are studied alongside duplex ones (e.g., EN 1.4362 and EN 1.4462). The calculated environmental impacts are the Global Warming Potential (GWP) and Primary Energy Demand (PED). The production, manufacturing, transport, use including maintenance activities, and end-of-life (burdens and credits) phases are included in the life cycle assessment (LCA). The maintenance activities consist of the required replacements of stainless steel piping during the lifespan of the WWTP. Thus, the service lives of the pipes included in the considered WWTP environment are determined based on long-term corrosion prediction models (power law), which predict the evolution of pit or crevice depth as a function of time. The model parameters are estimated based on own experimental results, supplemented by the existing literature. The corrosion rates determine the number and frequency of replacements, i.e., define the different scenarios of maintenance. The LCA, LCC and corrosion prediction models are then combined into a user-friendly tool, which can be used in industry for an appropriate grade selection for pipes in a WWTP environment. The tool includes several degrees of freedom such as piping distribution, water pressure, chloride content, replacement criteria, etc. The results show that using duplex stainless steel grade EN 1.4462 leads to lower GWP and PED at the end of the WWTP's service life of 40 years. This is mainly due to multiple replacements of the system's parts in wastewater with high levels of chloride (>3000 ppm) if more conventional austenitic stainless steel alloys such as EN 1.4404 are used. Leaner duplex stainless steel grades were also included in this LCC assessment. The duplex grade EN 1.4062 showed the lowest total LCC, thanks to its leaner chemical composition (i.e., lower nickel content) combined with good localized corrosion resistance.


Subject(s)
Stainless Steel , Water Purification , Animals , Corrosion , Life Cycle Stages , Steel
2.
Materials (Basel) ; 14(11)2021 May 28.
Article in English | MEDLINE | ID: mdl-34071568

ABSTRACT

The effects of cathodic polarisation switch-off on the passivation of AISI 304L stainless steel in air and its crevice corrosion susceptibility in 3.5 wt.% NaCl aqueous electrolyte were investigated. Scanning Kelvin probe (SKP) data showed that the oxide film is significantly destabilised and the rate of steel passivation in air is slowed down. Thermal desorption analysis (TDA) highlighted that hydrogen absorption is proportional to the applied cathodic current density. A special crevice corrosion set-up was designed to realise simultaneous reproducible monitoring of potential and galvanic current to study the impact of prior cathodic polarisation on crevice corrosion onset.

3.
Front Microbiol ; 10: 170, 2019.
Article in English | MEDLINE | ID: mdl-30792705

ABSTRACT

Microorganisms can increase the open-circuit potential of stainless steel immersed in seawater of several hundred millivolts in a phenomenon called ennoblement. It raises the chance of corrosion as the open-circuit potential may go over the pitting corrosion potential. Despite the large impact of the ennoblement, no unifying mechanisms have been described as responsible for the phenomenon. Here we show that the strict electrotroph bacterium "Candidatus Tenderia electrophaga" is detected as an ennoblement biomarker and is only present at temperatures at which we observe ennoblement. This bacterium was previously enriched in biocathode systems. Our results suggest that "Candidatus Tenderia electrophaga," and its previously described extracellular electron transfer metabolism coupled to oxygen reduction activity, could play a central role in modulating stainless steel open-circuit potential and consequently mediating ennoblement.