Your browser doesn't support javascript.
loading
Show: 20 | 50 | 100
Results 1 - 2 de 2
Filter
Add more filters










Database
Language
Publication year range
1.
J Mech Behav Biomed Mater ; 110: 103875, 2020 10.
Article in English | MEDLINE | ID: mdl-32957185

ABSTRACT

The chemistry of resin-based dental adhesives is critical for its interaction with dental tissues and long-term bonding stability. Changes in dental adhesives composition influences the materials' key physical-chemical properties, such as rate and degree of conversion, water sorption, solubility, flexural strength and modulus, and cohesive strength and improves the biocompatibility to dental tissues. Maintaining a suitable reactivity between photoinitiators and monomers is important for optimal properties of adhesive systems, in order to enable adequate polymerisation and improved chemical, physical and biological properties. The aim of this article is to review the current state-of-the-art of dental adhesives, and their chemical composition and characteristics that influences the polymerisation reaction and subsequent materials properties and performance.


Subject(s)
Dental Bonding , Dentin-Bonding Agents , Adhesives , Composite Resins , Dental Cements , Dentin , Materials Testing , Resin Cements
2.
Dent Mater ; 36(10): 1356-1364, 2020 10.
Article in English | MEDLINE | ID: mdl-32888725

ABSTRACT

OBJECTIVE: This study investigated viscosity and thermal kinetics of 10 selected preheated restorative resin composites and the effect of ultrasound energy on film thickness. METHODS: A range of different resin composites was tested: Charisma Diamond, IPS Empress Direct, Enamel Plus HRi, Essentia, Estelite Omega, Filtek Z100, Filtek Z350 XT, Gradia, TPH Spectrum and VisCalor. A flowable resin composite (Opallis Flow) and two resin cements (RelyX Veneer, Variolink Esthetic LC) also were tested. Viscosity (Pa s) was measured at 37 °C and 69 °C (preheating temperature) using a rheometer. Film thickness (µm) was measured before and after application of ultrasound energy. Temperature loss within resin composite following preheating (°C/s) was monitored. Data were statistically analyzed (α = 0.05). RESULTS: Viscosity at 69 °C was lower than at 37 °C for all materials except the flowable resin composite. Preheating reduced viscosity between 47% and 92% for the restorative resin composites, which were generally more viscous than the flowable materials. Film thickness varied largely among materials. All preheated resin composites had films thicker than 50 µm without ultrasound energy. Application of ultrasound reduced film thickness between 21% and 49%. Linear and nonlinear regressions did not identify any relationship between filler loading, viscosity, and/or film thickness. All materials showed quick temperature reduction following preheating, showing maximum temperature loss rates after approximately 10 s. SIGNIFICANCE: Distinct restorative resin composites react differently to preheating, affecting viscosity and film thickness. The overall performance of the preheating technique depends on proper material selection and use of ultrasound energy for reducing film thickness.


Subject(s)
Composite Resins , Motion Pictures , Dental Enamel , Kinetics , Materials Testing , Resin Cements , Viscosity
SELECTION OF CITATIONS
SEARCH DETAIL
...