The hydroxyl groups on the cellulose macromolecular chain cause the cellulose surface to have strong reactivity. In this study, 1H, 1H, 2H, 2H-perfluorodecyltriethoxysilane (PDOTES) was used to modify cellulose to improve its triboelectric properties, and a triboelectric nanogenerator (TENG) was assembled. The introduction of fluorine groups reduced the surface potential of cellulose and turned it into a negative phase, which enhanced the ability to capture electrons. The electrical properties increased by 30% compared with unmodified cellulose. According to the principles of TENGs, a self-powered human-wearable device was designed using PDOTES-paper, which could detect movements of the human body, such as walking and running, and facilitated a practical method for the preparation of efficient wearable sensors.

2.
Polymers (Basel) ; 13(5)2021 Mar 04.
Article in English | MEDLINE | ID: mdl-33806542

ABSTRACT

Hydrogen peroxide chemo-mechanical pulp (APMP), sulfonated chemo-mechanical pulp (SCMP), and chemical thermomechanical pulp (CTMP) were used as raw materials to explore the effects of hydrogen peroxide (HP), Fenton pretreatment (FP), and ethanol pretreatment (EP) on the enzymatic hydrolysis of high-yield bamboo mechanical pulp (HBMP). The surface lignin distribution and contents of different HBMPs were determined using confocal laser scanning microscopy (CLSM) and X-ray photoelectron spectroscopy (XPS). The correlation between the surface lignin and the enzymatic hydrolysis of HBMP was also investigated. The residue of enzymatic hydrolysis was used to adsorb methylene blue (MB). The results showed that the cracks and fine fibers on the surface of APMP, SCMP, and CTMP increased after FP, when compared to HP and EP. The total removal content of hemicellulose and lignin in SCMP after FP was higher than with HP and EP. Compared to SCMP, the crystallinity increased by 15.4%, and the surface lignin content of Fenton-pretreated SCMP decreased by 11.7%. The enzymatic hydrolysis efficiency of HBMP after FP was higher than with HP and EP. The highest enzymatic hydrolysis of Fenton-pretreated SCMP was 49.5%, which was higher than the enzymatic hydrolysis of Fenton-pretreated APMP and CTMP. The removal rate of MB reached 94.7% after the adsorption of the enzymatic hydrolysis residue of SCMP. This work provides an effective approach for a high value-added utilization of high-yield bamboo pulp.