ABSTRACT

The optimization of alternative materials in concrete production continues to garner considerable attention in order to meet sustainability goals and supplement natural materials. Portland limestone cement (PLC) and municipal solid waste incineration (MSWI) bottom ash (BA) have been proposed separately as green cement and coarse aggregate supplement in low-strength concrete production, creating sustainable products and alternative disposal scenario for a waste material. This study discusses the impact of advanced ash processing techniques on aggregates and presents the performance of concrete incorporating both of these products with PLC for the first time. Two sources of MSWI BA were investigated, one as-produced (TMR) and one processed with novel advanced metals recovery (AMR). The AMR process reduced total Al content in ash compared to TMR (20,500 vs 17,000 mg/kg), though not aluminum oxide content, as the AMR process targets metallic aluminum. A composition study on both aggregates supports a reduction in ferrous and non-ferrous metals following the AMR process. All control and test mixes met 28-day compressive strength requirements (17 Mpa). Both AMR and TMR MSWI BA-amended concretes yielded compressive strengths below control specimens (no ash) ranging from 17 to 23 MPa, with little to no difference observed dependent on MSWI BA processing. The life-cycle discussion supports benefits deriving from supplementing naturally mined materials and recovering ferrous and nonferrous metals with the AMR process.

2.
Chemosphere ; 336: 139198, 2023 Sep.
Article in English | MEDLINE | ID: mdl-37315860

ABSTRACT

Concentrations of 25 inorganic elements were measured in both bulk ash and individual ash components from residuals at three municipal solid waste incineration (MSWI) facilities in the US (two combined ash (CA) and one bottom ash (BA)). Concentrations were assessed based on particle size and component to understand the contribution from each fraction. The results found that among facilities, the finer size fractions contained elevated concentrations of trace elements of concern (As, Pb, Sb) when compared to the coarse fraction, but concentrations varied among facilities depending on the type of ash and differences in advanced metals recovery processes. This study focused on several constituents of potential concern, As, Ba, Cu, Pb, and Sb, and found that the main components of MSWI ash (glass, ceramic, concrete, and slag) are sources of these elements in the ash streams. For many elements, concentrations were significantly higher in CA bulk and component fractions opposed to BA streams. An acid treatment procedure and scanning electron microscopy/energy-dispersive x-ray spectroscopy analysis revealed that some elements, such as As in concrete, are result of the inherent properties of the component, but other elements, such as Sb, form on the surface during or after incineration and can be removed. Some Pb and Cu concentrations were attributed to inclusions in the glass or slag introduced into the material during the incineration process. Understanding the contributions of each ash component provides critical information for developing strategies to reduce trace element concentrations in ash streams to promote reuse opportunities.


Subject(s)
Metals, Heavy , Refuse Disposal , Trace Elements , Incineration , Solid Waste/analysis , Trace Elements/analysis , Lead/analysis , Coal Ash/chemistry , Metals, Heavy/analysis
3.
Sci Total Environ ; 851(Pt 1): 158163, 2022 Dec 10.
Article in English | MEDLINE | ID: mdl-35988635

ABSTRACT

Phosphogypsum (PG) samples from four distinct sources in the Southeastern US were analyzed to explore the variation in total metal content between newly generated (fresh) PG and PG disposed of in phosphogypsum stacks for different lengths of time (stack). Fresh PG exhibited greater total metal concentrations relative to stack PG, including those identified in the literature as important from a risk assessment perspective (As, Cd, Co, Cr, Cu, Pb, and Zn). The pH varied between fresh and stack PG, with some stack samples exhibiting lower pH than fresh samples, however the relationship between pH and age of sample was not linear. Stack samples with pH values similar to fresh samples possessed lower concentrations of total inorganic metals than fresh samples suggesting that process water drainage and stack location play an important role in the reusability of PG as they can affect the pH of stack PG and total inorganic metal concentrations. Overall observations show that stacking PG for three or more years prior to beneficial reuse provides a construction material with lower total metal concentrations than fresh PG.


Subject(s)
Metals, Heavy , Trace Elements , Cadmium , Calcium Sulfate , Environmental Monitoring , Lead , Metals, Heavy/analysis , Phosphorus , Water