Environ Sci Pollut Res Int ; 30(46): 102986-103000, 2023 Oct.
Artículo en Inglés | MEDLINE | ID: mdl-37674070

RESUMEN

The photocatalytic efficiency of some semiconductors depends mainly on their morphological, optical, and structural properties, which can be modified by varying the calcination temperature. In order to evaluate how these properties change, as a function of temperature in a AA'BB'O3 perovskite material, La0.9Sr0.1Fe0.8Co0.2O3±Î´ (LSFC) was synthesized by the Pechini method and calcined at different temperatures (600 °C, 700 °C, 800 °C, and 900 °C). All the samples were characterized structurally, morphologically, and optically by XRD, SEM, and UV-Vis spectroscopy. Additionally, specific surface area and pore size distribution were calculated by BET and BHJ methods. LSFC was evaluated as photocatalyst material, estimating the degradation of reactive black 5 (RB5), employing as irradiation source UV light and sunlight. The obtained results display a clear tendency between the photoactivity and the heat treatment: degradation percentage decreases as the calcination temperature increases mainly due to the crystal and grain size and, furthermore, loss of porosity and the decrease in surface area, affecting the photocatalytic activity (98%, 95%, 74%, and 50% degradation, respectively). All the ceramic samples follow a pseudo-first-order reaction.

2.
Materials (Basel) ; 16(6)2023 Mar 11.
Artículo en Inglés | MEDLINE | ID: mdl-36984148

RESUMEN

Ba0.92Ca0.08Ti0.95Zr0.05O3 (BCZT8-5) ceramic materials have been scarcely studied as lead-free piezo/ferroelectrics despite their enhanced Curie temperature (>100 °C) with respect to most studied BCZT compositions. In this work, homogeneous dense BCZT8-5 ceramics with grain size in the range of 20 µm, and optimum ferroelectric, dielectric, and electromechanical performance, were prepared by the mixed oxides route using moderate synthesis (1250 °C-2 h) and sintering (1400 °C-2 h) conditions. Thickness-poled thin disks and monomodal shear plate resonators were used for the determination of piezoelectric coefficients, coupling factors, elastic, and dielectric permittivity coefficients, including all losses, by iterative analysis of impedance curves at resonance. Furthermore, the thermal evolution of the piezoelectric characteristics at resonance was determined to assess the enhanced working range of the ceramics (≈100 °C). Ferroelectric hysteresis loops and strains vs. electric-field butterfly loops were also measured and showed soft behavior with Ec = 2 kV/cm, Pr = 12 µC/cm2 after a maximum applied field of 3 kV was used. The ceramics showed a high endurance of P-E cycles to electrical fatigue up to 107 cycles. Moreover, dielectric properties as a function of temperature were also accomplished and showed nearly normal ferroelectric behavior, characteristic of samples with low crystallographic disorder. Overall, these ceramics showed high sensitivity and higher stability than other currently studied BCZT compositions.

3.
Materials (Basel) ; 13(7)2020 Apr 03.
Artículo en Inglés | MEDLINE | ID: mdl-32260151

RESUMEN

Coupling between electrically excited electromechanical resonances of piezoelectric ceramics is undesirable for the purpose of their characterization, since the material models correspond to monomodal resonances. However, coupling takes place quite often and it is unavoidable at the shear resonance of standard in-plane poled and thickness-excited rectangular plates. The piezoelectric coefficient e15, the elastic compliance s55E and the dielectric permittivity component ε11S for a piezoelectric ceramic can be determined, including all losses, using the automatic iterative method of analysis of the complex impedance curves for the shear mode of an appropriated resonator. This is the non-standard, thickness-poled and longitudinally excited, shear plate. In this paper, the automatic iterative method is modified. The purpose is to be able to deal with the analysis of the impedance curves of the non-standard plate as the periodic phenomena of coupling and decoupling of the main shear resonance and other resonances takes place. This happens when the thickness of the plate is reduced, and its aspect ratio (width of the excitation (w)/thickness for poling (t)) is increased. In this process, the frequency of the shear resonance also increases and meets those of other plate modes periodically. We aim to obtain the best approach for the shear properties of near coupling and to reveal both their validity and the limitations of the thus-obtained information. Finally, we use a plate of a Ba0.85Ca0.15Ti0.90Zr0.10O3 eco-piezoceramic as a case study.

4.
Materials (Basel) ; 9(1)2016 Jan 02.
Artículo en Inglés | MEDLINE | ID: mdl-28787822

RESUMEN

The search for electroceramic materials with enhanced ferro-pyro-piezoelectric properties and revealing the perovskite type structure has been the objective of a significant number of manuscripts reported in the literature. This has been usually carried out by proposing the synthesis and processing of new compounds and solid solution series. In this work, several methods to obtain ferro-pyro-piezoelectric families of materials featuring the well-known ABO3 perovskite structure (or related) such as BaTiO3, Ba1-xCaxTi1-yZryO3, (Bi0.5Na0.5)TiO3, (K0.5Na0.5)NbO3 and their solid solutions with different cations either in the A or B positions, are presented. For this kind of materials, the challenge for obtaining a single phase compound with a specific grain size and morphology and, most importantly, with the adequate stoichiometry, will also be discussed. The results reviewed herein will be discussed in terms of the tendency of working with softer conditions, i.e., lower temperature and shorter reaction times, also referred to as soft-chemistry.