Different programs in a microwave oven were selected to dry several gypsum products. A type III dental stone (Moldano), a type IV high-strength dental stone (Glastone) and a type III partial denture casting investment (Multi-vest) were selected. Specimens of the products were dried by microwave radiation set at the lowest and highest power levels for 5 and 15 minutes. The dried specimens were tested at intervals of 2, 4, 24, and 48 hours for compressive strength. Specimens dried in ambient room air were used as the control group. A statistical analysis of the test results was performed with Student's t-test at p < or = 0.05 level. Microwave radiation at the highest power level resulted in a decrease in the compressive strength of type IV dental stone (Glastone), whereas the values of the other gypsum products did not differ at any time interval from values attained for the air-dried specimens. The 2-hour low power test of the investment (Multi-vest) had a higher compressive strength than the air-dried specimens after 24 hours.


Assuntos
Sulfato de Cálcio/efeitos da radiação , Revestimento para Fundição Odontológica/efeitos da radiação , Micro-Ondas , Ar , Sulfato de Cálcio/química , Fenômenos Químicos , Físico-Química , Equipamentos Odontológicos , Dessecação , Dureza , Umidade , Teste de Materiais
11.
Istanbul Univ Dishekim Fak Derg ; 2(3): 254-84, 1968 Sep.
Artigo em Turco | MEDLINE | ID: mdl-5265407
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...