Your browser doesn't support javascript.
loading
Mostrar: 20 | 50 | 100
Resultados 1 - 17 de 17
Filtrar
Mais filtros










Base de dados
Intervalo de ano de publicação
1.
Eur Heart J Digit Health ; 4(4): 283-290, 2023 Aug.
Artigo em Inglês | MEDLINE | ID: mdl-37538147

RESUMO

Aims: Over the last ten years, virtual Fractional Flow Reserve (vFFR) has improved the utility of Fractional Flow Reserve (FFR), a globally recommended assessment to guide coronary interventions. Although the speed of vFFR computation has accelerated, techniques utilising full 3D computational fluid dynamics (CFD) solutions rather than simplified analytical solutions still require significant time to compute. Methods and results: This study investigated the speed, accuracy and cost of a novel 3D-CFD software method based upon a graphic processing unit (GPU) computation, compared with the existing fastest central processing unit (CPU)-based 3D-CFD technique, on 40 angiographic cases. The novel GPU simulation was significantly faster than the CPU method (median 31.7 s (Interquartile Range (IQR) 24.0-44.4s) vs. 607.5 s (490-964 s), P < 0.0001). The novel GPU technique was 99.6% (IQR 99.3-99.9) accurate relative to the CPU method. The initial cost of the GPU hardware was greater than the CPU (£4080 vs. £2876), but the median energy consumption per case was significantly less using the GPU method (8.44 (6.80-13.39) Wh vs. 2.60 (2.16-3.12) Wh, P < 0.0001). Conclusion: This study demonstrates that vFFR can be computed using 3D-CFD with up to 28-fold acceleration than previous techniques with no clinically significant sacrifice in accuracy.

2.
J Mech Behav Biomed Mater ; 138: 105572, 2023 02.
Artigo em Inglês | MEDLINE | ID: mdl-36435033

RESUMO

Joint replacements have become one of the most common orthopedic procedures due to the significant demands of retaining functional mobility. While these procedures are of great value to patients, there are some limitations. Durability is the most important limitation associated with joint replacement that needs to be addressed due to the increasing number of younger patients. Titanium is a commonly used implant material which has high biocompatibility, high strength-to-density ratio, and high corrosion resistance. However, current titanium implants have poor wear resistance which shortens their lifespan. In this study, microscale dimples with four different dimple shapes (circular, triangular, square, and star) of similar sizes to the pores found in natural articular cartilage were fabricated on titanium disks to improve implant lubrication and reduce wear. Biotribology tests were performed on dimpled and non-dimpled titanium disks in a condition similar to that inside of a patient's body. It was shown that dimpling the titanium disks optimized the lubricant film formation and decreased the wear rate significantly while also reducing the coefficient of friction (COF). The star-shaped dimples had the lowest COF and almost no detectable wear after 8 h of testing. To investigate whether dimpling increased bacterial colonization due to increased surface area, and to determine whether any increase could be limited by coating with antibacterial materials, bacterial colonization with Staphylococcus aureus was tested with non-dimpled and star-shaped dimpled titanium disks with and without coating with polydopamine (PDA), silver (Ag) nanoparticles (NPs), and PDA + Ag NPs. It was found that dimpling did not increase bacterial colonization, and that coating with PDA, Ag NPs, or PDA + Ag NPs did not decrease bacterial colonization. Nevertheless, we conclude that star-shaped dimpled titanium surfaces have potential utility as more durable orthopedic implants.


Assuntos
Nanopartículas , Titânio , Humanos , Antibacterianos , Fricção , Staphylococcus aureus , Propriedades de Superfície , Materiais Revestidos Biocompatíveis
3.
PLoS One ; 17(8): e0272169, 2022.
Artigo em Inglês | MEDLINE | ID: mdl-35917312

RESUMO

Microneedle patches are a promising source for transdermal diffusion of macromolecules and are designed to painlessly penetrate the skin. In this study, a biodegradable chitosan microneedle patch to deliver meloxicam for managing pain in cattle was tested. The potential of reuse of the polymeric solution to fabricate the patches, optimization of fabrication, morphological analysis of the microneedle patch and analysis of preservation of the chemical composition after sterilization were evaluated. In-vitro analysis consisted of studying in-vitro penetration mechanical properties, compression testing analysis of microneedle patch, and in-vitro drug release analysis. In-vivo studies were performed to analyze the dissolution capability of the microneedle patch. Results regarding the physical characteristics, chemical composition, and mechanical properties confirmed that rheological properties of the chitosan solution, present significant differences over time, demonstrating that reusing the solution on the fourth day results in failure patches. Morphological characteristics and chemical composition studies revealed that the process of sterilization (ethylene oxide gas) needed for implanting the patches into the skin did not affect the properties of microneedle patches. In-vitro studies showed that approximately 33.02 ± 3.88% of the meloxicam was released over 7 days. A full penetration of the microneedles into the skin can be obtained by applying approximately 3.2 N. In-vivo studies demonstrated that microneedle patches were capable of swelling and dissolving, exhibiting a dissolution percentage of more than 50% of the original height of microneedle after 7 days. No abnormal tissue, swelling, or inflammation was observed in the implanted area. The results of this work show that chitosan biodegradable microneedle patches may be useful to deliver meloxicam to improve pain management of cattle with positive effects for commercial manufacturing.


Assuntos
Quitosana , Administração Cutânea , Animais , Bovinos , Quitosana/química , Sistemas de Liberação de Medicamentos/métodos , Meloxicam/farmacologia , Agulhas , Dor/tratamento farmacológico , Dor/veterinária , Manejo da Dor , Pele , Adesivo Transdérmico
4.
J Funct Biomater ; 12(2)2021 May 01.
Artigo em Inglês | MEDLINE | ID: mdl-34062752

RESUMO

To understand the possible lubricant mechanism in ceramic-on-ceramic hip joint prostheses, biochemical reactions of the synovial fluid and the corresponding frictional coefficients were studied. The experiments were performed in a hip joint simulator using the ball-on-cup configuration with balls and cups made from two types of ceramics, BIOLOX®forte and BIOLOX®delta. Different lubricants, namely albumin, γ-globulin, hyaluronic acid and three model synovial fluids, were studied in the experiments and Raman spectroscopy was used to analyze the biochemical responses of these lubricants at the interface. BIOLOX®delta surface was found less reactive to proteins and model fluid lubricants. In contrast, BIOLOX®forte ball surface has shown chemisorption with both proteins, hyaluronic acid and model fluids imitating total joint replacement and osteoarthritic joint. There was no direct correlation between the measured frictional coefficient and the observed chemical reactions. In summary, the study reveals chemistry of lubricant film formation on ceramic hip implant surfaces with various model synovial fluids and their components.

5.
J Bodyw Mov Ther ; 22(3): 757-760, 2018 Jul.
Artigo em Inglês | MEDLINE | ID: mdl-30100309

RESUMO

BACKGROUND: It has been established that Hyper-pronation of the foot may lead to postural changes in the lower limbs, with a resultant pelvic ante-version, and a subsequent risk of development of low back pain. However, the association between the presence of a hyper-pronated foot and the severity of disability in low back pain is currently not known. OBJECTIVES: The purpose of this study was to examine whether the presence of a hyper-pronated foot has any impact on the degree of severity of disability (functional status) in patients with non-specific low back pain. METHODS: An observational study was conducted in an outpatient setting, where patients diagnosed as having non-specific low back pain were included. The degree of severity of disability was measured using the Modified Oswestry Low Back Pain Disability Questionnaire, and the foot hyper-pronation was assessed with the execution of the Navicular Drop test. Descriptive statistics and Linear regression analyses were conducted. RESULTS: Of the 71 patients included, 14 demonstrated having a unilateral hyper-pronation of the foot. The mean scores for the functional status and hyper-pronation of the foot were 37.15 (SD = 10.40) and 6.06 (SD = 3.42) respectively. An association was not found between the severity of disability and the presence of foot hyper-pronation (B = .87, p = .78). CONCLUSIONS: Hyper-pronation of the foot could lead to the development of non-specific low back pain, but the degree of severity of the disability is not influenced by the presence of a hyper-pronated foot. The alterations in lower limb mechanics leading to back pain are a complex issue, and thus needs further research.


Assuntos
Pé/fisiopatologia , Dor Lombar/diagnóstico , Pronação , Índice de Gravidade de Doença , Adulto , Feminino , Humanos , Extremidade Inferior/fisiopatologia , Masculino , Pessoa de Meia-Idade , Medição da Dor/métodos , Suporte de Carga/fisiologia
6.
J Mech Behav Biomed Mater ; 81: 120-129, 2018 05.
Artigo em Inglês | MEDLINE | ID: mdl-29501964

RESUMO

This study evaluates the impact of dimple shapes on lubricant film formation in artificial hip joints. Micro-dimples with 20-50 µm lateral size and 1 ±â€¯0.2 µm depths were fabricated on CrCoMo hip joint femoral heads using a picosecond laser. Tribological studies were performed using a pendulum hip joint simulator to apply continuous swing flexion-extension motions. The results revealed a significantly enhanced lubricant film thickness (≥ 500 nm) with micro-dimpled prosthesis heads at equilibrium position after the lubricant film has fully developed. The average lubricant film thickness of dimpled prostheses with square- and triangular-shaped dimple arrays over time is about 3.5 that of the non-dimpled prosthesis (204 nm). Remarkably, the prosthesis with square-shaped dimple arrays showed a very fast lubricant film formation reaching their peak values within 0.5 s of pendulum movement, followed by prosthesis with triangular-shaped dimple arrays with a transition period of 42.4 s. The fully developed lubricant film thicknesses (≥ 700 nm) are significantly higher than the surface roughness (≈ 25 nm) demonstrating a hydrodynamic lubrication. Hardly any scratches appeared on the post-experimental prosthesis with square-shaped dimple array and only a few scratches were found on the post-experimental prosthesis with triangular-shaped dimple arrays. Thus, prostheses with square-shaped dimple arrays could be a potential solution for durable artificial hip joints.


Assuntos
Prótese de Quadril , Fenômenos Mecânicos , Líquido Sinovial/metabolismo , Animais , Bovinos
7.
J Mech Behav Biomed Mater ; 79: 314-323, 2018 03.
Artigo em Inglês | MEDLINE | ID: mdl-29353775

RESUMO

The number of revision joint replacements has been increasing substantially over the last few years. Understanding their failure mechanism is extremely important for improving the design and material selection of current implants. This study includes ten retrieved and four new mildly cross-linked ultra-high molecular weight polyethylene (UHMWPE) acetabular liners. Among them, most of the prostheses (n = 5) were reported to be revised and replaced due to aseptic loosening, followed by painful joint (n = 2), dislocation (n = 1), intra articular ossification (n = 1), combination of wear (liner) and osteolysis (stem) (n=1). Surface deviations (wear, material inflation and roughness), oxidative degradation and change of material properties were measured using micro-computed tomography (micro-CT) scan, 3D laser scanning microscopy, raman spectroscopy and nanoindentation, respectively. Prostheses having eccentric worn areas had much higher linear wear rates (228.01 ± 35.51µm/year) compared to that of centrically worn prostheses (96.71 ± 10.83µm/year). Oxidation index (OI) showed similar trends to the surface penetration depth. Among them, sample 10 exhibited the highest OI across the contact area and the rim of the cup liner. It also had the lowest hardness/elasticity ratio. Overall, wear and creep, oxidative degradation and reduced hardness/elasticity ratio all contributed to the premature failure of the UHMWPE acetabular cup liners.


Assuntos
Acetábulo/cirurgia , Artroplastia de Quadril , Prótese de Quadril , Desenho de Prótese , Idoso , Feminino , Humanos , Masculino , Teste de Materiais , Pessoa de Meia-Idade , Polietilenos/química , Falha de Prótese
8.
J Mech Behav Biomed Mater ; 72: 192-199, 2017 08.
Artigo em Inglês | MEDLINE | ID: mdl-28500998

RESUMO

Coefficient of friction (COF) tests were conducted on 28-mm and 36-mm-diameter hip joint prostheses for four different material combinations, with or without the presence of Ultra High Molecular Weight Polyethylene (UHMWPE) particles using a novel pendulum hip simulator. The effects of three micro dimpled arrays on femoral head against a polyethylene and a metallic cup were also investigated. Clearance played a vital role in the COF of ceramic on polyethylene and ceramic on ceramic artificial hip joints. Micro dimpled metallic femoral heads yielded higher COF against a polyethylene cup; however, with metal on metal prostheses the dimpled arrays significantly reduced the COF. In situ images revealed evidence that the dimple arrays enhanced film formation, which was the main mechanism that contributed to reduced friction.


Assuntos
Cerâmica/análise , Fricção , Prótese de Quadril , Teste de Materiais , Polietilenos/análise , Interface Osso-Implante , Articulação do Quadril , Humanos , Próteses Articulares Metal-Metal
9.
J Mech Behav Biomed Mater ; 68: 51-61, 2017 04.
Artigo em Inglês | MEDLINE | ID: mdl-28152443

RESUMO

Six types of diamond-like carbon (DLC) coatings with zirconium (Zr)-containing interlayers on titanium alloy (Ti-6Al-4V) were investigated for improving the biotribological performance of orthopedic implants. The coatings consist of three layers: above the substrate a layer stack of 32 alternating Zr and ZrN sublayers (Zr:ZrN), followed by a layer comprised of Zr and DLC (Zr:DLC), and finally a N-doped DLC layer. The Zr:ZrN layer is designed for increasing load carrying capacity and corrosion resistance; the Zr:DLC layer is for gradual transition of stress, thus enhancing layer adhesion; and the N-doped DLC layer is for decreasing friction, squeaking noises and wear. Biotribological experiments were performed in simulated body fluid employing a ball-on-disc contact with a Si3N4 ball and a rotational oscillating motion to mimic hip motion in terms of gait angle, dynamic contact pressures, speed and body temperature. The results showed that the Zr:DLC layer has a substantial influence on eliminating delamination of the DLC from the substrates. The DLC/Si3N4 pairs significantly reduced friction coefficient, squeaking noise and wear of both the Si3N4 balls and the discs compared to those of the Ti-6Al-4V/Si3N4 pair after testing for a duration that is equivalent to one year of hip motion in vivo.


Assuntos
Carbono/química , Teste de Materiais , Próteses e Implantes , Titânio/química , Zircônio/química , Ligas , Corrosão , Diamante , Prótese de Quadril , Humanos , Propriedades de Superfície , Suporte de Carga
10.
J Mech Behav Biomed Mater ; 59: 586-595, 2016 06.
Artigo em Inglês | MEDLINE | ID: mdl-27085502

RESUMO

This study investigates the durability of functional diamond-like carbon (DLC) coated titanium alloy (Ti-6Al-4V) under edge loading conditions for application in artificial hip joints. The multilayered (ML) functional DLC coatings consist of three key layers, each of these layers were designed for specific functions such as increasing fracture strength, adapting stress generation and enhancing wear resistance. A 'ball-on-disk' multi-directional wear tester was used in the durability test. Prior to the wear testing, surface hardness, modulus elasticity and Raman intensity were measured. The results revealed a significant wear reduction to the DLC coated Ti-6Al-4V disks compared to that of non-coated Ti-6Al-4V disks. Remarkably, the counterpart Silicon Nitride (Si3N4) balls also yielded lowered specific wear rate while rubbed against the coated disks. Hence, the pairing of a functional multilayered DLC and Si3N4 could be a potential candidate to orthopedics implants, which would perform a longer life-cycle against wear caused by edge loading.


Assuntos
Diamante/química , Prótese de Quadril , Teste de Materiais , Titânio/química , Ligas , Carbono , Humanos , Desenho de Prótese , Propriedades de Superfície
11.
J Mech Behav Biomed Mater ; 45: 121-31, 2015 May.
Artigo em Inglês | MEDLINE | ID: mdl-25704181

RESUMO

This study investigates a tribological performance of diamond like carbon (DLC) coated micro dimpled prosthesis heads against ceramic cups in a novel pendulum hip joint simulator. The simulator enables determining friction coefficient and viscous effects of a concave shaped specimen interface (conformal contact). Two types of DLC such as hydrogenated amorphous carbon (a-C:H) and tetrahedral amorphous carbon (Ta-C) and one set of micro dimple (diameter of 300µm, depth of 70µm, and pitch of 900µm) were fabricated on metallic prosthesis heads. The experiment results reveal a significant friction coefficient reduction to the 'dimpled a-C:H/ceramic' prosthesis compared to a 'Metal (CoCr)/ceramic' prosthesis because of their improved material and surface properties and viscous effect. The post-experiment surface analysis displays that the dimpled a-C:H yielded a minor change in the surface roughness, and generated a larger sizes of wear debris (40-200nm sized, equivalent diameter), a size which could be certainly stored in the dimple, thus likely to reducing their possible third body abrasive wear rate. Thus, dimpled a:C-H can be used as a 'metal on ceramic hip joint interface', whereas the simulator can be utilized as an advanced bio-tribometer.


Assuntos
Diamante , Teste de Materiais , Fenômenos Mecânicos , Ortopedia , Próteses e Implantes , Fricção , Articulação do Quadril , Propriedades de Superfície
12.
Sci Technol Adv Mater ; 16(3): 035002, 2015 Jun.
Artigo em Inglês | MEDLINE | ID: mdl-27877803

RESUMO

Osteoarthritis-oriented synovial fluid (OASF), i.e., that typical of a patient with osteoarthritis, has different physical and biological characteristics than bovine serum (BS), a lubricant widely used in biotribological investigations. Micro-dimpled and diamond-like carbon- (DLC) coated surfaces are key emerging interfaces for orthopedic implants. In this study, tribological performances of dimpled surfaces, with and without DLC coating, have been investigated under both BS and OASF. The friction tests were performed utilizing a pin on a disk tribometer, whereas contact pressure, speed, and temperature were simulated to a 'medium walking gait' of hip joint conditions. The mechanical properties of the specimen and the physical properties of the lubricant were characterized before the friction test. Raman analysis was conducted to identify the coating condition both before and after the test. The DLC-coated dimpled surface showed maximum hardness and residual stress. A DLC-coated dimpled surface under an OASF lubricated condition yielded a lower friction coefficient and wear compared to those of plain and dimpled specimens. The higher graphitization of coated materials with increasing load was confirmed by Raman spectroscopy.

13.
Sci Technol Adv Mater ; 16(4): 045002, 2015 Aug.
Artigo em Inglês | MEDLINE | ID: mdl-27877822

RESUMO

The concentration of biological components of synovial fluid (such as albumin, globulin, hyaluronic acid, and lubricin) varies between healthy persons and osteoarthritis (OA) patients. The aim of the present study is to compare the effects of such variation on tribological performance in a simulated hip joint model. The study was carried out experimentally by utilizing a pin-on-disk simulator on ceramic-on-ceramic (CoC) and ceramic-on-polyethylene (CoP) hip joint implants. The experimental results show that both friction and wear of artificial joints fluctuate with the concentration level of biological components. Moreover, the performance also varies between material combinations. Wear debris sizes and shapes produced by ceramic and polyethylene were diverse. We conclude that the biological components of synovial fluid and their concentrations should be considered in order to select an artificial hip joint to best suit that patient.

14.
J Biomed Mater Res B Appl Biomater ; 103(5): 1002-12, 2015 Jul.
Artigo em Inglês | MEDLINE | ID: mdl-25220737

RESUMO

Diamond like carbon (DLC) is applied as a thin film onto substrates to obtain desired surface properties such as increased hardness and corrosion resistance, and decreased friction and wear rate. Microdimple is an advanced surface modification technique enhancing the tribological performance. In this study, DLC coated microdimples were fabricated on hip prosthesis heads and their mechanical, material and surface properties were characterized. An Electro discharge machining (EDM) oriented microdrilling was utilized to fabricate a defined microdimple array (diameter of 300 µm, depth of 70 µm, and pitch of 900 µm) on stainless steel (SS) hip prosthesis heads. The dimpled surfaces were then coated by hydrogenated amorphous carbon (a-C:H) and tetrahedral amorphous carbon (Ta-C) layers by using a magnetron sputtering technology. A preliminary tribology test was conducted on these fabricated surfaces against a ceramic ball in simulated hip joint conditions. It was found that the fabricated dimples were perpendicular to the spherical surfaces and no cutting-tools wear debris was detected inside the individual dimples. The a-C:H and Ta-C coatings increased the hardness at both the dimple edges and the nondimpled region. The tribology test showed a significant reduction in friction coefficient for coated surfaces regardless of microdimple arrays: the lowest friction coefficient was found for the a-C:H samples (µ = 0.084), followed by Ta-C (µ = 0.119), as compared to the SS surface (µ = 0.248).


Assuntos
Carbono/química , Materiais Revestidos Biocompatíveis/química , Prótese de Quadril , Humanos , Propriedades de Superfície
15.
PLoS One ; 9(6): e100028, 2014.
Artigo em Inglês | MEDLINE | ID: mdl-24927127

RESUMO

Cricket has over the years gained much popularity in Asia, thus the number of cricket players has also grown in tandem. However, cricket players are not as fortunate as other athletes as they do not always have a standard cricket infrastructure to practice; therefore, the injury prevalence is expected to be high. Unfortunately, very few studies have been conducted to investigate the nature and pattern of cricket injuries prevalent to cricketers in this region. Therefore, a prospective cohort injury surveillance study was conducted during the Asian Cricket Council (ACC) Under-19 Elite Cup held in June 2013 in order to gather more data on the type of injuries sustained by cricket players. Overall, 31 injuries occurred to 28 players throughout the tournament, of which 7 injuries happened during practice sessions. The overall injury incidence rate (IIR) was 292.0 per 10,000 player hours (95% CI 176.9-407.1) and 10.4 per 10,000 balls faced and 2.6 per 1000 overs bowled delivered during batting and bowling, respectively. Injuries to the lower limb (IIR: 146; 95% CI 1.8-98.2) were the most frequent, followed by injuries to the upper limb (97.3;95% CI 30.2-164.5) and to the trunk and back (IIR: 36.5;95% CI 0.0-77.7). Sprain/strains (IIR 109.5;95% CI 38.4-180.7) to muscle/tendon and joint/ligament were the most commonly reported nature of injury. This is the first study investigating injury incidence among the players of the ACC. It provides an overview of injuries sustained by elite players' under-19 years of age from 10 Asian countries. The overall IIR is similar to earlier studies conducted in well-established cricket playing nations.


Assuntos
Traumatismos em Atletas/epidemiologia , Esportes , Entorses e Distensões/epidemiologia , Esportes Juvenis , Adolescente , Ásia , Criança , Pré-Escolar , Comportamento Competitivo , Humanos , Incidência , Masculino , Esportes/estatística & dados numéricos , Adulto Jovem , Esportes Juvenis/estatística & dados numéricos
16.
Sci Technol Adv Mater ; 15(1): 014402, 2014 Feb.
Artigo em Inglês | MEDLINE | ID: mdl-27877638

RESUMO

Coatings such as diamond-like carbon (DLC) and titanium nitride (TiN) are employed in joint implants due to their excellent tribological properties. Recently, graphite-like carbon (GLC) and tantalum (Ta) have been proven to have good potential as coating as they possess mechanical properties similar to bones-high hardness and high flexibility. The purpose of this systematic literature review is to summarize the coating techniques of these four materials in order to compare their mechanical properties and tribological outcomes. Eighteen studies published between January 2000 and February 2013 have met the inclusion criteria for this review. Details of their fabrication parameters, material and mechanical properties along with the tribological outcomes, such as friction and wear rate, were identified and are presented in a systematic way. Although experiment conditions varied, we conclude that Ta has the lowest wear rate compared to DLC, GLC and TiN because it has a lower wear rate with high contact pressure as well as higher hardness to elasticity ratio. However, a further tribology test is needed in an environment which replicates artificial joints to confirm the acceptability of these findings.

17.
Materials (Basel) ; 7(2): 980-1016, 2014 Feb 10.
Artigo em Inglês | MEDLINE | ID: mdl-28788496

RESUMO

Wear debris, of deferent sizes, shapes and quantities, generated in artificial hip and knees is largely confined to the bone and joint interface. This debris interacts with periprosthetic tissue and may cause aseptic loosening. The purpose of this review is to summarize and collate findings of the recent demonstrations on debris characterization and their biological response that influences the occurrence in implant migration. A systematic review of peer-reviewed literature is performed, based on inclusion and exclusion criteria addressing mainly debris isolation, characterization, and biologic responses. Results show that debris characterization largely depends on their appropriate and accurate isolation protocol. The particles are found to be non-uniform in size and non-homogeneously distributed into the periprosthetic tissues. In addition, the sizes, shapes, and volumes of the particles are influenced by the types of joints, bearing geometry, material combination, and lubricant. Phagocytosis of wear debris is size dependent; high doses of submicron-sized particles induce significant level of secretion of bone resorbing factors. However, articles on wear debris from engineered surfaces (patterned and coated) are lacking. The findings suggest considering debris morphology as an important parameter to evaluate joint simulator and newly developed implant materials.

SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...