Waste Manag ; 155: 8-18, 2023 Jan 01.
Artigo em Inglês | MEDLINE | ID: mdl-36335774

RESUMO

Full-component pyrolysis has been proven to be a prospective method for the disposal of organic matters and the cathode material reduction of spent LiNixCoyMnzO2 (NCM) lithium-ion batteries (LIBs). However, the kinetics of the full-component pyrolysis of spent NCM LIBs is still unclear. This work represents the first attempt to study the kinetics of different stages of full-component pyrolysis of NCM LIBs based on isoconversional method to guide the recycling of spent LIBs. Pyrolysis process was divided into four stages in accordance to the main weight loss temperature ranges and the classical Kissinger-Akahira-Sunose and Flynn-Wall-Ozawa kinetics models were employed to calculate the activation energy (E) in each stage. The main physicochemical reactions were clarified though in situ analysis, and the average E in the four stages was determined: (I) The volatilization of electrolytes occurred in the temperature range of 100-200 °C with the E of 98.6 kJ/mol. (II) The decomposition of organic matters and the preliminary reduction of cathode material transpired in the temperature range of 400-500 °C with the E of 227.2 kJ/mol. (III) The further reduction of NiO and CoO occurred from 650 to 800 °C with the E of 258.8 kJ/mol. (Ⅳ) The reduction of MnO took place from 850 to 1000 °C with the E of 334.9 kJ/mol. The recycling strategies based on full-component pyrolysis of spent NCM LIBs was accordingly proposed. During pyrolysis, the cathode material was gradually reduced and the pyrolytic products can be controlled through temperature regulation.

SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...