J Arthroplasty ; 19(4): 532-6, 2004 Jun.
Artigo em Inglês | MEDLINE | ID: mdl-15188120

RESUMO

A 68-year-old patient underwent revision surgery for recurrent dislocation of a ceramic-on-polyethylene uncemented hip arthroplasty implanted 6 months previously. The aluminum oxide femoral head was found to have titanium deposition measuring 5 by 10 mm in an area articulating with the highly cross-linked polyethylene liner. The liner was observed to possess severe scratching produced by articulation with the titanium deposited on the ceramic head. Despite improved scratch resistance of ceramic-bearing surfaces, irregularities introduced by metallic deposition after recurrent dislocation can damage a highly cross-linked polyethylene liner.


Assuntos
Artroplastia de Quadril , Luxação do Quadril/cirurgia , Osteólise/etiologia , Falha de Prótese , Idoso , Óxido de Alumínio , Humanos , Masculino , Microscopia Eletrônica de Varredura , Osteólise/diagnóstico por imagem , Polietileno , Radiografia , Reoperação , Propriedades de Superfície , Titânio
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...