Int J Prosthodont ; 28(5): 487-9, 2015.
Artigo em Inglês | MEDLINE | ID: mdl-26340008

RESUMO

PURPOSE: Ceramic defects in porcelain-fused-to-metal (PFM) restorations may depend on framework alloy type. This study assessed ceramic defects on cobalt-chromium- (Co-Cr-) and gold-platinum- (Au-Pt-) based PFM restorations. MATERIALS AND METHODS: In this study, 147 Co-Cr-based and 168 Au-Pt-based PFM restorations inserted between 1998 and 2010 (139 patients) were examined for ceramic defects. Detected defects were assigned to three groups according to clinical defect relevance. RESULTS: Ceramic defect rates (Co-Cr-based: 12.9%; Au-Pt-based: 7.2%) revealed no significant difference but a strong statistical trend (U test, P = .082). Most defects were of little clinical relevance. CONCLUSIONS: Co-Cr PFM restorations may be at higher risk for ceramic defects compared to Au-Pt-based restorations.


Assuntos
Cerâmica/química , Ligas de Cromo/química , Coroas , Falha de Restauração Dentária , Prótese Parcial Fixa , Ligas de Ouro/química , Ligas Metalo-Cerâmicas/química , Platina/química , Adulto , Idoso , Idoso de 80 Anos ou mais , Polimento Dentário/métodos , Reparação em Prótese Dentária , Facetas Dentárias , Reparação em Dentadura , Feminino , Seguimentos , Humanos , Masculino , Pessoa de Meia-Idade , Retratamento , Estudos Retrospectivos , Propriedades de Superfície
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...