Nature ; 617(7961): 507-512, 2023 05.
Artigo em Inglês | MEDLINE | ID: mdl-37198308

RESUMO

Electric vehicles demand high charge and discharge rates creating potentially dangerous temperature rises. Lithium-ion cells are sealed during their manufacture, making internal temperatures challenging to probe1. Tracking current collector expansion using X-ray diffraction (XRD) permits non-destructive internal temperature measurements2; however, cylindrical cells are known to experience complex internal strain3,4. Here, we characterize the state of charge, mechanical strain and temperature within lithium-ion 18650 cells operated at high rates (above 3C) by means of two advanced synchrotron XRD methods: first, as entire cross-sectional temperature maps during open-circuit cooling and second, single-point temperatures during charge-discharge cycling. We observed that a 20-minute discharge on an energy-optimized cell (3.5 Ah) resulted in internal temperatures above 70 °C, whereas a faster 12-minute discharge on a power-optimized cell (1.5 Ah) resulted in substantially lower temperatures (below 50 °C). However, when comparing the two cells under the same electrical current, the peak temperatures were similar, for example, a 6 A discharge resulted in 40 °C peak temperatures for both cell types. We observe that the operando temperature rise is due to heat accumulation, strongly influenced by the charging protocol, for example, constant current and/or constant voltage; mechanisms that worsen with cycling because degradation increases the cell resistance. Design mitigations for temperature-related battery issues should now be explored using this new methodology to provide opportunities for improved thermal management during high-rate electric vehicle applications.

SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...