Biomed Mater Eng ; 28(2): 169-185, 2017.
Artigo em Inglês | MEDLINE | ID: mdl-28372269

RESUMO

OBJECTIVE: The purpose of this study was to evaluate the effect of double-application coats and times on microtensile bond strength (µTBS) and adhesive-dentin interfaces created by dentin adhesive systems after 6 months of storage in water. MATERIALS AND METHODS: Two-hundred sixteen extracted non-carious human third molars were selected for the study. Single-Bond Universal (SU) and All-Bond Universal (AU), Adper Easy One (Eo) Self-Etch adhesive and Adper Single-Bond 2 (Sb) etch-and-rinse adhesive were applied to a flat dentin surface using three methods (1): dentin adhesives were applied as recommended by the manufacturers; (2): two consecutive coats of dentin adhesives were applied before photo-polymerization; and (3): a single coat of adhesive was applied but with twice the manufacturers recommended application time. Microtensile bond strength was determined either immediately or after 6 months of water storage. Data were analyzed using one-way analysis of variance and Tukey's post-hoc tests. RESULTS: At 24 h, groups 1, 2, and 3 exhibited statistically similar results for all dentin adhesive systems. For AU-Er, group 3 showed significantly higher bond strength than all group of AU-Se after 6 months. CONCLUSION: Universal adhesives seemed more stable against water degradation than traditional two-step etch-and-rinse and all-in-one systems within the 6-month period.


Assuntos
Adesivos/química , Materiais Revestidos Biocompatíveis/química , Adesivos Dentinários/química , Bis-Fenol A-Glicidil Metacrilato/química , Cimentos Dentários/química , Humanos , Teste de Materiais , Dente Serotino/química , Polimerização , Cimentos de Resina/química , Estresse Mecânico , Resistência à Tração , Água/química
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...