Bioresour Technol ; 100(1): 292-8, 2009 Jan.
Artigo em Inglês | MEDLINE | ID: mdl-18650083

RESUMO

In this study, contributions of hemicellulose, cellulose and lignin to the mass and the porous properties of chars and activated carbons from various lignocellulosic materials were studied. A predictive calculation was established using the experimental results obtained for the three components separately to evaluate the carbonization and activation yields and their respective contributions to the chars and to the subsequent activated carbons of various precursors in term of weight fraction. These equations were validated. The results showed that lignin can be considering as being the major contributor of all chars and activated carbons. Besides, the evolution of the mean pore size versus the specific porous volume showed that each component contributes to the porosity of chars and activated carbons whatever is its weight contribution.


Assuntos
Celulose/química , Carvão Vegetal/química , Lignina/química , Modelos Químicos , Polissacarídeos/química , Simulação por Computador , Peso Molecular , Porosidade , Vapor
2.
J Phys Chem B ; 110(7): 3055-60, 2006 Feb 23.
Artigo em Inglês | MEDLINE | ID: mdl-16494308

RESUMO

(129)Xe NMR has been used to study a series of homologous activated carbons obtained from a KOH-activated pitch-based carbon molecular sieve modified by air oxidation/pyrolysis cycles. A clear correlation between the pore size of microporous carbons and the (129)Xe NMR of adsorbed xenon is proposed for the first time. The virial coefficient delta(Xe)(-)(Xe) arising from binary xenon collisions varied linearly with the micropore size and appeared to be a better probe of the microporosity than the chemical shift extrapolated to zero pressure. This correlation was explained by the fact that the xenon collision frequency increases with increasing micropore size. The chemical shift has been shown to vary very little with temperature (less than 9 ppm) for xenon trapped inside narrow and wide micropores. This is indicative of a smooth xenon-surface interaction potential.