1.
Polymers (Basel) ; 14(21)2022 Nov 02.
Artigo em Inglês | MEDLINE | ID: mdl-36365676

RESUMO

This paper illustrates a study of the thermal oxidation of several epoxy amine networks. Oxidation was followed at the molecular scale using Fourier Transform InfraRed spectroscopy (FTIR) and at the macromolecular scale using tensile tests. FTIR showed the major formation of amides, while tensile tests showed the progressive increase in the elastic modulus (~0.5 GPa for room temperature Young modulus) and decrease in ultimate strain and volumic energy for failure (assessed using the integrals of stress-strain curves). Both ultimate strain and volumic energy were divided by more than two. Linear correlations between oxidation trackers (amide concentration) and changes in mechanical parameters are presented and discussed.

2.
Chemosphere ; 288(Pt 1): 132364, 2022 Feb.
Artigo em Inglês | MEDLINE | ID: mdl-34600007

RESUMO

The need for personal protective equipment increased exponentially in response to the Covid-19 pandemic. To cope with the mask shortage during springtime 2020, a French consortium was created to find ways to reuse medical and respiratory masks in healthcare departments. The consortium addressed the complex context of the balance between cleaning medical masks in a way that maintains their safety and functionality for reuse, with the environmental advantage to manage medical disposable waste despite the current mask designation as single-use by the regulatory frameworks. We report a Workflow that provides a quantitative basis to determine the safety and efficacy of a medical mask that is decontaminated for reuse. The type IIR polypropylene medical masks can be washed up to 10 times, washed 5 times and autoclaved 5 times, or washed then sterilized with radiations or ethylene oxide, without any degradation of their filtration or breathability properties. There is loss of the anti-projection properties. The Workflow rendered the medical masks to comply to the AFNOR S76-001 standard as "type 1 non-sanitory usage masks". This qualification gives a legal status to the Workflow-treated masks and allows recommendation for the reuse of washed medical masks by the general population, with the significant public health advantage of providing better protection than cloth-tissue masks. Additionally, such a legal status provides a basis to perform a clinical trial to test the masks in real conditions, with full compliance with EN 14683 norm, for collective reuse. The rational reuse of medical mask and their end-of-life management is critical, particularly in pandemic periods when decisive turns can be taken. The reuse of masks in the general population, in industries, or in hospitals (but not for surgery) has significant advantages for the management of waste without degrading the safety of individuals wearing reused masks.


Assuntos
COVID-19 , Pandemias , Humanos , Máscaras , Equipamento de Proteção Individual , SARS-CoV-2
3.
Polymers (Basel) ; 13(23)2021 Nov 25.
Artigo em Inglês | MEDLINE | ID: mdl-34883610

RESUMO

In the context of the SARS-CoV2 pandemic and because of the surgical and FFP2 mask (equivalent to the American N95 masks) shortages, studies on efficient sterilization protocols were initiated. As sterilization using irradiation is commonly used in the medical field, this method was among those that were evaluated. In this work, we tested irradiation under vacuum and under air (under both γ-rays and e-beams), but also, for acceptance purposes, undertook washing prior to the e-beam irradiation sterilization process. This article deals with the modifications induced by the sterilization processes at the molecular and the macromolecular scales on an FFP2 mask. Fourier transform infrared spectroscopy in attenuated total reflectance mode, size-exclusion chromatography and thermal-desorption-gas chromatography-mass spectrometry were used to characterize possible damage to the materials. It appeared that the modifications induced by the different sterilization processes under vacuum were relatively tenuous and became more significant when irradiation was performed using γ-rays under air.

4.
J Mech Behav Biomed Mater ; 115: 104286, 2021 03.
Artigo em Inglês | MEDLINE | ID: mdl-33383378

RESUMO

This study aimed at determining an optimum polymerization pressure for Polymer Infiltrated Ceramic Network (PICN) blocks by characterizing the conversion degree (DC) and the viscoelastic properties of experimental PICN blocks polymerized at 90 °C under various high pressures followed or not by post-cure treatment (PC). Near infrared analysis and dynamic mechanical analysis were used to characterize DC and viscoelastic properties of sixteen PICN: one control (thermo-cured) and fifteen experimental groups (one thermo-cured followed by PC and fourteen high pressure polymerized PICN, in the range of 50-350 MPa without and with PC). Conversion degree of high pressure polymerized PICN blocks without post curing displays an optimum between 100 and 150 MPa resulting in an improved E' and Tg. Post curing induces a higher DC with a controversial effect on thermomechanical properties. The results suggested that 100-150 MPa without PC is an optimum polymerization parameter, resulting in PICN blocks with significantly better DC, Tg, E'.


Assuntos
Desenho Assistido por Computador , Polímeros , Cerâmica , Teste de Materiais , Polimerização , Propriedades de Superfície
5.
Chem Phys Lipids ; 165(7): 753-9, 2012 Oct.
Artigo em Inglês | MEDLINE | ID: mdl-23026153

RESUMO

This study deals with oxidation kinetics of three unsaturated fatty esters: methyl oleate, methyl linoleate and methyl linolenate at temperatures ranging from 90 to 150 °C. The reaction was monitored by chemiluminescence. A kinetic model was derived from a simple mechanistic scheme, in which initiation is due to hydroperoxides decomposition, whereas propagation results from the abstraction of the most labile hydrogen and termination results only from the bimolecular combination of peroxyl radicals. Analysis of induction period duration indicated that hydroperoxides mainly decompose by a bimolecular process. The model well predicts the main features of the experimental chemiluminescence curves. Kinetic parameters of the three unsaturated fatty esters were assessed from inverse method and discussed.