Biomaterials ; 11(7): 495-500, 1990 Sep.
Artigo em Inglês | MEDLINE | ID: mdl-2242398

RESUMO

Short-duration, cyclically loaded, axial, fretting corrosion tests were designed and performed to compare the fretting behaviour of different metal Howmedica universal heads connected to coated and uncoated metal cone taper spigots. Concurrent axial push-on and pull-off taper friction tests were also performed. There was no measurable fretting debris found in any test and SEM studies of the contact surfaces showed no evidence of fretting. It is concluded that no significant, long-term fretting corrosion of the Vitalium Co-Cr-Mo heads on the Vitallium or uncoated Ti-6AI-4V spigots, nor of the Orthinox stainless steel heads on the Orthinox spigots, is likely to occur in vivo.


Assuntos
Prótese de Quadril , Teste de Materiais , Metais , Corrosão , Desenho de Prótese , Falha de Prótese , Aço Inoxidável , Propriedades de Superfície , Vitálio
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...