Storage effect on the shear bond strength of adhesive systems
Konno, Alysson Noriyuki Kajishima; Sinhoreti, Mário Alexandre Coelho; Consani, Simonides; Sobrinho, Lourenço Correr; Consani, Rafael Leonardo Xediek.
Afiliación
  • Konno, Alysson Noriyuki Kajishima; Universidade Estadual de Campinas. Faculty of Dentistry of Piracicaba. Discipline of Dental Materials. Piracicaba. BR
  • Sinhoreti, Mário Alexandre Coelho; Universidade Estadual de Campinas. Faculty of Dentistry of Piracicaba. Discipline of Dental Materials. Piracicaba. BR
  • Consani, Simonides; Universidade Estadual de Campinas. Faculty of Dentistry of Piracicaba. Discipline of Dental Materials. Piracicaba. BR
  • Sobrinho, Lourenço Correr; Universidade Estadual de Campinas. Faculty of Dentistry of Piracicaba. Discipline of Dental Materials. Piracicaba. BR
  • Consani, Rafael Leonardo Xediek; Universidade Estadual de Campinas. Faculty of Dentistry of Piracicaba. Discipline of Dental Materials. Piracicaba. BR
Braz. dent. j ; Braz. dent. j;14(1): 42-47, June 2003. ilus, tab
Article en En | LILACS | ID: lil-340488
Biblioteca responsable: BR1.1
ABSTRACT
The purpose of this study was to evaluate the effects of storage (1 day, 3 months and 6 months) on the shear bond strength of five adhesive systems on bovine dentin substrate. One hundred and fifty bovine incisors were flattened until areas of a minimum of 5 mm in diameter were exposed. A round area of 4 mm in diameter was marked on the dentin to be treated with the following adhesive systems Clearfil Liner Bond 2V (CLB2V), Scotchbond Multi Purpose Plus (SBMP), Optibond Solo (SOLO), Prime & Bond NT (PBNT) and Etch & Prime 3.0 (E&P). To perform the test, a composite restoration (Z100) was made in a cylindrical shape on the treated surface. After the storage period in distilled water at 37ºC, the samples were tested on an Instron testing machine. Results were submitted to ANOVA and Tukey's test at 5 percent significance level. SBMP, PBNT and E&P were statistically similar at all storage times (p>0.05). CLB2V demonstrated the highest mean shear bond strength at 3 months which was not significantly different at 6 months (p>0.05). In addition, CLB2V had the highest means at all times tested. SOLO had the lowest mean shear bond strength at 6 months, which was statistically lower than means at 3 months and 1 day (p<0.05)
Asunto(s)
Texto completo: 1 Colección: 01-internacional Base de datos: LILACS Asunto principal: Circonio / Recubrimiento Dental Adhesivo / Recubrimientos Dentinarios / Dióxido de Silicio / Dentina Límite: Animals Idioma: En Revista: Braz. dent. j Asunto de la revista: ODONTOLOGIA Año: 2003 Tipo del documento: Article País de afiliación: Brasil Pais de publicación: Brasil
Texto completo: 1 Colección: 01-internacional Base de datos: LILACS Asunto principal: Circonio / Recubrimiento Dental Adhesivo / Recubrimientos Dentinarios / Dióxido de Silicio / Dentina Límite: Animals Idioma: En Revista: Braz. dent. j Asunto de la revista: ODONTOLOGIA Año: 2003 Tipo del documento: Article País de afiliación: Brasil Pais de publicación: Brasil