Your browser doesn't support javascript.
loading
Long-Term Stable Dispersion of Multiwalled Carbon Nanotubes by Peroxydisulfate upon Ultrasonication Activation.
He, Jinglei; He, Xin; Shen, Xiaofang; Yan, Chuanhao; Yu, Xuefeng; Zhang, Jinlong; Zhu, Benzhan; Huang, Chunhua; Liu, Junfeng; Wang, Xilong.
Afiliación
  • He J; Laboratory for Earth Surface Processes, College of Urban and Environmental Sciences, Peking University, Beijing, 100871, China.
  • He X; Laboratory for Earth Surface Processes, College of Urban and Environmental Sciences, Peking University, Beijing, 100871, China.
  • Shen X; College of Environmental Science and Engineering, Suzhou University of Science and Technology, Suzhou, 215009, China.
  • Yan C; Laboratory for Earth Surface Processes, College of Urban and Environmental Sciences, Peking University, Beijing, 100871, China.
  • Yu X; Laboratory for Earth Surface Processes, College of Urban and Environmental Sciences, Peking University, Beijing, 100871, China.
  • Zhang J; Laboratory for Earth Surface Processes, College of Urban and Environmental Sciences, Peking University, Beijing, 100871, China.
  • Zhu B; Research Center for Eco-Environmental Sciences, Chinese Academy of Sciences, Beijing, 100085, China.
  • Huang C; Research Center for Eco-Environmental Sciences, Chinese Academy of Sciences, Beijing, 100085, China.
  • Liu J; Laboratory for Earth Surface Processes, College of Urban and Environmental Sciences, Peking University, Beijing, 100871, China.
  • Wang X; Laboratory for Earth Surface Processes, College of Urban and Environmental Sciences, Peking University, Beijing, 100871, China.
Small ; : e2400675, 2024 Aug 16.
Article en En | MEDLINE | ID: mdl-39150058
ABSTRACT
Poor dispersibility of carbon nanotubes greatly hinders their practical applications. Herein, a long-term stable dispersion of multiwalled carbon nanotubes (MWCNTs) in peroxydisulfate (PDS) is achieved. MWCNTs at 40 mg L-1 are completely dispersed by PDS upon ultrasonication (US/PDS) within 64 min and a stable dispersion is maintained at least 20 days. Mechanistically, US created defects on the nanomaterial and PDS-origin free radicals attacked these defects to introduce O-containing moieties (─OH and ─COOH). Interestingly, dispersion efficiency of MWCNTs by US/PDS initially at pH 7 and 3.8 is comparable, but lower than that initially at pH 12. Both •OH and SO4 •- are produced under alkaline condition, while SO4 •- is the dominant free radicals initially at pH 7 and 3.8 during the whole dispersion period. Stronger dispersion of MWCNTs initially at pH 12 resulted from greater amounts of O-containing moieties mainly in ─OH (46.32%) rather than ─COOH (24.19%) form. This differential more strongly promotes MWCNTs-water interaction via hydrogen bonding, thereby enhancing the dispersion. Notably, no significant mass loss of MWCNTs occurred during dispersion. Overall, the developed method achieves long-term stable dispersion of MWCNTs in a manner that can significantly extend their applications.