Your browser doesn't support javascript.
loading
Photocatalytic Degradation of Diclofenac Using Al2O3-Nd2O3 Binary Oxides Prepared by the Sol-Gel Method.
Casillas, José Eduardo; Campa-Molina, Jorge; Tzompantzi, Francisco; Carbajal Arízaga, Gregorio Guadalupe; López-Gaona, Alejandro; Ulloa-Godínez, Sandra; Cano, Mario Eduardo; Barrera, Arturo.
Afiliação
  • Casillas JE; Departamento de Ciencias Básicas, Centro Universitario de la Ciénega, Universidad de Guadalajara, Av. Universidad, No. 1115, Ocotlán C.P. 47820, Jalisco, Mexico.
  • Campa-Molina J; Departamento de Electrónica, Universidad de Guadalajara, Marcelino García Barragán 1422, Guadalajara C.P. 44430, Jalisco, Mexico.
  • Tzompantzi F; Departamento de Química, Universidad Autónoma Metropolitana-Iztapalapa, San Rafael Atlixco 189, Ciudad de México C.P. 09340, Mexico.
  • Carbajal Arízaga GG; Departamento de Química, Universidad de Guadalajara, Marcelino García Barragán 1422, Guadalajara C.P. 44430, Jalisco, Mexico.
  • López-Gaona A; Departamento de Química, Universidad Autónoma Metropolitana-Iztapalapa, San Rafael Atlixco 189, Ciudad de México C.P. 09340, Mexico.
  • Ulloa-Godínez S; Departamento de Electrónica, Universidad de Guadalajara, Marcelino García Barragán 1422, Guadalajara C.P. 44430, Jalisco, Mexico.
  • Cano ME; Departamento de Ciencias Básicas, Centro Universitario de la Ciénega, Universidad de Guadalajara, Av. Universidad, No. 1115, Ocotlán C.P. 47820, Jalisco, Mexico.
  • Barrera A; Departamento de Ciencias Básicas, Centro Universitario de la Ciénega, Universidad de Guadalajara, Av. Universidad, No. 1115, Ocotlán C.P. 47820, Jalisco, Mexico.
Materials (Basel) ; 13(6)2020 Mar 16.
Article em En | MEDLINE | ID: mdl-32188051
This paper reports the sol-gel synthesis of Al2O3-Nd2O3 (Al-Nd-x; x = 5%, 10%, 15% and 25% of Nd2O3) binary oxides and the photodegradation of diclofenac activated by UV light. Al-Nd-based catalysts were analyzed by N2 physisorption, XRD, TEM, SEM, UV-Vis and PL spectroscopies. The inclusion of Nd2O3 in the aluminum oxide matrix in the 10-25% range reduced the band gap energies from 3.35 eV for the γ-Al2O3 to values as low as 3.13-3.20 eV, which are typical of semiconductor materials absorbing in the UV region. γ-Al2O3 and Al-Nd-x binary oxides reached more than 92.0% of photoconverted diclofenac after 40 min of reaction. However, the photocatalytic activity in the diclofenac degradation using Al-Nd-x with Nd2O3 contents in the range 10-25% was improved with respect to that of γ-Al2O3 at short reaction times. The diclofenac photoconversion using γ-Al2O3 was 63.0% at 10 min of UV light exposure, whereas Al-Nd-15 binary oxide reached 82.0% at this reaction time. The rate constants determined from the kinetic experiments revealed that the highest activities in the aqueous medium were reached with the catalysts with 15% and 25% of Nd2O3, and these compounds presented the lowest band gap energies. The experimental results also demonstrated that Nd2O3 acts as a separator of charges favoring the decrease in the recombination rate of electron-hole pairs.