Effects of curing temperature on the compressive strength and microstructure of copper tailing-based geopolymers.
Tian, Xiang; Xu, Wangyang; Song, Shaoxian; Rao, Feng; Xia, Ling.
Afiliação
  • Tian X; Hubei Key Laboratory of Mineral Resources Processing and Environment, Luoshi Road 122, Wuhan, Hubei, 430070, China; CONACYT Instituto de Investigación en Metalurgia y Materiales, Universidad Michoacana de San Nicolás de Hidalgo, Morelia, Mich., 58030, Mexico.
  • Xu W; Hubei Key Laboratory of Mineral Resources Processing and Environment, Luoshi Road 122, Wuhan, Hubei, 430070, China.
  • Song S; Hubei Key Laboratory of Mineral Resources Processing and Environment, Luoshi Road 122, Wuhan, Hubei, 430070, China. Electronic address: shaoxian@uaslp.mx.
  • Rao F; School of Zijin Mining, Fuzhou University, Fuzhou, Fujian, 350108, China; CONACYT Instituto de Investigación en Metalurgia y Materiales, Universidad Michoacana de San Nicolás de Hidalgo, Morelia, Mich., 58030, Mexico. Electronic address: fengrao@fzu.edu.cn.
  • Xia L; Hubei Key Laboratory of Mineral Resources Processing and Environment, Luoshi Road 122, Wuhan, Hubei, 430070, China.
Chemosphere ; 253: 126754, 2020 Aug.
Article em En | MEDLINE | ID: mdl-32302914
This study sought to analyze the effect of curing temperature on mechanical strength and microstructure of a copper tailing-based geopolymer via scanning electron microscopy (SEM), HCl extraction, nuclear magnetic resonance (NMR), and X-ray diffraction (XRD). The distribution of gel formed in geopolymers tended to be uniform with increasing curing temperature from 25 to 80 °C. Moreover, the percentage of Si sites in C-S-H and N-A-S-H gels increased from 62.08% to 78.94% and more tetrahedral [AlO4] was incorporated into the tetrahedron [SiO4] backbone, leading to an increase of compressive strength from 10.2 to 39.6 MPa. When the curing temperature was increased to 120 °C, the percentage of Si sites in C-S-H and N-A-S-H gel decreased to 69.52%, and the compressive strength decreased to 27.5 MPa. Moderately elevated curing temperature promoted the dissolution of aluminosilicate while curing temperatures above 80 °C hindered it. Excessive curing temperature led to a decrease in the geopolymer alkaline medium.
Assuntos
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Gerenciamento de Resíduos / Materiais de Construção / Cobre / Silicatos de Alumínio / Resíduos Industriais Idioma: En Revista: Chemosphere Ano de publicação: 2020 Tipo de documento: Article País de afiliação: México País de publicação: Reino Unido

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Gerenciamento de Resíduos / Materiais de Construção / Cobre / Silicatos de Alumínio / Resíduos Industriais Idioma: En Revista: Chemosphere Ano de publicação: 2020 Tipo de documento: Article País de afiliação: México País de publicação: Reino Unido